Physical Properties | Metric | English | Comments |
---|---|---|---|
Viscosity | 300 cP @Temperature 25.0 °C |
300 cP @Temperature 77.0 °F |
Hardener |
Protective Coating PC-Rot Terminator® Epoxy Wood Consolidant Description: PC-Rot Terminator® is designed to strengthen decayed or rotted wood. The mixture is a low viscosity liquid that penetrates porous surfaces filling and sealing voids with an epoxy that .. |
|||
Viscosity | 300 cP @Shear Rate 10.0 1/s, Temperature 280 °C |
300 cP @Shear Rate 10.0 1/s, Temperature 536 °F |
|
Solvay TECHNYL® A 218 V30 BK 34 NG PA66, 30% glass fiber, DRY Description: TECHNYL® A 218 V30 Black 34 NG is a polyamide 66, reinforced with 30% of glass fiber, heat stabilized, for injection molding. The product is available in black color.Benefits: This p.. |
|||
Viscosity | 300 cP @Shear Rate 100 1/s, Temperature 275 °C |
300 cP @Shear Rate 100 1/s, Temperature 527 °F |
|
Solvay TECHNYL® A 218 V30 Black 21 NHFE PA66, 30% glass fiber, DRY Description: TECHNYL® A 218 V30 BLACK 21NHFE is a polyamide 6.6, high flow, reinforced with 30% of glass fiber, heat stabilized, for injection molding. This product is available in black color.Be.. |
|||
Viscosity | 300 cP @Shear Rate 10.0 1/s, Temperature 280 °C |
300 cP @Shear Rate 10.0 1/s, Temperature 536 °F |
|
Solvay TECHNYL® A 218 V30 PA66, 30% glass fiber, DRY Description: TECHNYL® A 218 V30 is a polyamide 66, reinforced with 30% of glass fiber, heat stabilized, for injection molding. This product is available in natural and black colors.Benefits: The .. |
|||
Viscosity | 300 cP @Shear Rate 10.0 1/s, Temperature 280 °C |
300 cP @Shear Rate 10.0 1/s, Temperature 536 °F |
|
Solvay TECHNYL® A 218 V35 PA66, 35% glass fiber, DRY Description: TECHNYL® A 218 V35 is a polyamide 66, reinforced with 35% of glass fiber, heat stabilized, for injection molding. This product is available in natural and black colors.Benefits: The .. |
|||
Viscosity | 300 cP @Shear Rate 100 1/s, Temperature 260 °C |
300 cP @Shear Rate 100 1/s, Temperature 500 °F |
|
Solvay TECHNYL® C 218 V 30 PA6, 30% glass fiber, DRY Description: TECHNYL® C 218 V30 is a polyamide 6, heat stabilized, reinforced with 30% of glass fiber, for injection molding. This product is available in black color.Benefits: The product offers.. |
|||
Viscosity | 300 cP @Shear Rate 100 1/s, Temperature 230 °C |
300 cP @Shear Rate 100 1/s, Temperature 446 °F |
|
Solvay TECHNYLSTARâ„¢ S 60G1 V30 PA6, 30% glass filled, DRY Description: TECHNYLSTARâ„¢ S 60G1 V30 is a reinforced 30% GF organophosphorous flame retarded grade based on a patented high flow polyamide 6 resin (TechnylStar). This product is heat stabilized.. |
|||
Viscosity | 300 cP @Shear Rate 100 1/s, Temperature 250 °C |
300 cP @Shear Rate 100 1/s, Temperature 482 °F |
|
Solvay TECHNYLSTARâ„¢ SX 218 V50 PA6, 50% glass filled, DRY Description: TECHNYLSTARâ„¢ SX 218 V50 is based on a patented high flow polyamide 6 resin (Technylstar), heat stabilized, reinforced with 50% of glass fiber, for injection molding. This product i.. |
|||
Viscosity | 300 cP @Shear Rate 10.0 1/s, Temperature 280 °C |
300 cP @Shear Rate 10.0 1/s, Temperature 536 °F |
|
Solvay TECHNYL® A 218W V30 Natural PA66, 30% glass fiber, DRY Description: TECHNYL® A 218W V30 Nat is a polyamide 66, reinforced with 30% of glass fiber, heat stabilized, for injection molding. This product is available in natural color.Benefits: The produc.. |
|||
Viscosity | 300 cP @Temperature 37.8 °C |
300 cP @Temperature 100 °F |
|
BASF Pluracol® 1538 Slabstock Foam Polyol Description: Pluracol® 1538 polyol is intended for the production of Visco-Elastic foam typically formulated with another base product such as Pluracol 593 polyol. The combination of these two immi.. |
|||
Viscosity | 300 cP @Temperature 75.0 °C |
300 cP @Temperature 167 °F |
A Side |
ACC EP RAP 60 EPI Engineered Polymers Aliphatic Polyurea EP RAP 60 Aliphatic Polyurea, “Powered by Reactamine® Technology”, is a two component 100% solids, no VOC, coating (silicone optional) developed for UV stable (colorfast) polyurea flooring applic.. |
|||
Viscosity | 300 cP @Temperature 60.0 °C |
300 cP @Temperature 140 °F |
|
BASF Pluracol® SG-360 Rigid Polyol Description: Pluracol® SG-360 polyol is a clear, light colored, low viscosity, sucrose/glycerine polyol. Pluracol SG-360 contains no nitrogen. The medium functionality polyol, when combined with su.. |
|||
Viscosity | 300 cP @Shear Rate 100 1/s, Temperature 280 °C |
300 cP @Shear Rate 100 1/s, Temperature 536 °F |
|
Solvay TECHNYL® A 20 V25 PA66, 25% glass fiber, DRY Description: TECHNYL® A 20 V25 is a 25% glass fiber reinforced Red Phosphorous flame retarded grade based on a polyamide 66 resin. This product is heat stabiised for optimised injection moulding. T.. |
|||
Viscosity | 300 cP @Shear Rate 10.0 1/s, Temperature 275 °C |
300 cP @Shear Rate 10.0 1/s, Temperature 527 °F |
|
Solvay TECHNYL® A 218 V35 Black 21NHFE PA66, 35% glass fiber, DRY Description: TECHNYL® A 218 V35 BLACK 21NHFE is polyamide 6.6, high flow, reinforced with 35% glass fiber, heat stabilized, for injection molding. This product is available in black color.Benefits:.. |