Physical Properties | Metric | English | Comments |
---|---|---|---|
Viscosity | 290000 cP @Temperature 25.0 °C |
290000 cP @Temperature 77.0 °F |
ET538A, Epoxy Resin |
Permabond ET538 Epoxy Resin PERMABOND ET538 is a structural, room temperature curing epoxy adhesive that has excellent adhesion to a wide variety of surfaces such as wood, metal, ceramics and many plastic and composite materia.. |
|||
Viscosity | 290000 cP @Shear Rate 500 1/s, Temperature 275 °C |
290000 cP @Shear Rate 500 1/s, Temperature 527 °F |
ISO 11403-1 -2 |
DuPont Performance Polymers Zytel® 70G30HSL BK039B Nylon 66
(Unverified Data**) 30% Glass Reinforced Heat Stabilized Polyamide 66 Information provided by DuPont Performance Polymers |