Physical Properties | Metric | English | Comments |
---|---|---|---|
Viscosity | 248000 cP @Shear Rate 500 1/s, Temperature 295 °C |
248000 cP @Shear Rate 500 1/s, Temperature 563 °F |
ISO 11403-1 -2 |
DuPont Performance Polymers Rynite® 415HP NC010 Polyethylene Terephthalate (PET)
(Unverified Data**) 15% Glass Reinforced Polyethylene Terephthalate with Excellent Impact Resistance Rynite 415HP NC010 is a 15% glass reinforced modified polyethylene terephthalate improved for easy fast processing ov.. |
|||
Viscosity | 248000 cP @Shear Rate 500 1/s, Temperature 295 °C |
248000 cP @Shear Rate 500 1/s, Temperature 563 °F |
DAM; ISO 11443 |
DuPont Performance Polymers Zytel® 70G30HSLR NC010 Nylon 66
(Unverified Data**) Zytel® 70G30HSLR NC010 is a 30% glass fiber reinforced, heat stabilized, hydrolysis resistant polyamide 66 resin for injection molding.Information provided by DuPont Performance Polymers |
|||
Viscosity | 248000 cP @Shear Rate 500 1/s, Temperature 295 °C |
248000 cP @Shear Rate 500 1/s, Temperature 563 °F |
ISO 11403-1 -2 |
DuPont Performance Polymers Zytel® 70G35HSL NC010 Nylon 66
(Unverified Data**) 35% Glass Reinforced Heat Stabilized Polyamide 66 Zytel 70G35HSL NC010 is a 35% glass fiber reinforced heat stabilized polyamide 66 resin for injection molding.Information provided by DuPont Perform.. |