Physical Properties | Metric | English | Comments |
---|---|---|---|
Viscosity | 22 cP @Temperature 23.9 °C |
22 cP @Temperature 75.0 °F |
|
Paratherm Corporation Paratherm™ HR™ Heat Transfer Fluid Paratherm HR™ Heat Transfer Fluid is an alkylated-aromatic based heat transfer fluid formulated for closed loop liquid phase heating to 650°F in fired heaters and 675°F in waste heat recovery and.. |
|||
Viscosity | 22 cP @Temperature 30.0 °C |
22 cP @Temperature 86.0 °F |
5% wt Toluene Solution |
Kuraray SEPTON® S4044 Thermoplastic Rubber SEPTON® is a series of high performance thermoplastic rubbers developed by Kuraray Co. Ltd. using its isoprene technology. SEPTON® resins are hydrogenated styrenic block copolymers, which exhi.. |
|||
Viscosity | 22 - 50 cP @Time 241 sec |
22 - 50 cP @Time 0.0670 hour |
V-128-1 |
Solvay JAGUAR® 418 Surfactant Description: Nonyl Jaguar 418 is a carboxymethylhydroxypropyl guar with extremely low residue and dual cross-linking capability. When dispersed into water with agitation it will wet out and hydrate .. |
|||
Viscosity | 22 cP @Shear Rate 10000 1/s, Temperature 280 °C |
22 cP @Shear Rate 10000 1/s, Temperature 536 °F |
|
Solvay TECHNYL® A 205F PA66, DRY Description: TECHNYL ® A 205F is an unreinforced polyamide 66 for injection molding. It is available in natural color.Benefits: The product offers two main advantages: excellent filling qualities.. |
|||
Viscosity | 22 cP @Temperature 190 °C |
22 cP @Temperature 374 °F |
Melt (Unpolymerized resin); Cone and plate 10 1/s shear rate |
Cyclics CBT® 200 Thermoplastic Resin CBT® 200 resin melts to a water-like viscosity when heated, then polymerizes into the engineering thermoplastic resin polybutylene terephthalate (PBT). CBT 200 resin has a processing range between.. |