Physical Properties | Metric | English | Comments |
---|---|---|---|
Viscosity | 20000 cP @Shear Rate 11200 1/s, Temperature 200 °C |
20000 cP @Shear Rate 11200 1/s, Temperature 392 °F |
ASTM D3835 |
PolyOne Versaflex™ VDT 4132 Thermoplastic Elastomer (TPE) Versaflex™ VDT 4132 is designed to create vibration damping. - Excellent Vibration DampingRear = 350-370F Middle = 375-400F Front = 375-400F Nozzle = 365-380F Screw speed = 100-500rpmPurge thorough.. |
|||
Viscosity | 20000 cP @Temperature 25.0 °C |
20000 cP @Temperature 77.0 °F |
ET505A, Epoxy Resin |
Permabond ET505 Epoxy Resin PERMABOND ET505 is a two-part, 1:1 mixable epoxy adhesive. ET505 is a semi-flexible toughened epoxy adhesive with good adhesion to a variety of substrates such as wood, metal, ceramics and some plas.. |
|||
Viscosity | 20000 cP @Temperature 25.0 °C |
20000 cP @Temperature 77.0 °F |
ET515A, Epoxy Resin |
Permabond ET515 Epoxy Resin PERMABOND® ET515 is a 1:1 mixable epoxy adhesive. ET515 is a semi-flexible toughened adhesive with good adhesion to a variety of substrates such as wood, metal, ceramics and some plastics and compo.. |
|||
Viscosity | 20000 cP @Temperature 25.0 °C |
20000 cP @Temperature 77.0 °F |
at 20 rpm vibration |
Permabond F202 Anaerobic Retainer The unique 'toughening' process incorporated into Permabond® F202 gives this anaerobic adhesive excellent resistance to peel and impact forces. Primarily designed for use on metal surfaces, it is a.. |
|||
Viscosity | 20000 cP @Shear Rate 100000 1/s, Temperature 295 °C |
20000 cP @Shear Rate 100000 1/s, Temperature 563 °F |
|
DSM Arnite® AV2 390 XT PET GF50 50% Glass Reinforced, Applications with extremely narrow tolerances |
|||
Viscosity | 20000 cP @Shear Rate 100000 1/s, Temperature 250 °C |
20000 cP @Shear Rate 100000 1/s, Temperature 482 °F |
|
DSM Arnite® TM4 440 (PBT+PET)-MD20 20% Mineral Reinforced |
|||
Viscosity | 20000 cP @Shear Rate 100000 1/s, Temperature 230 °C |
20000 cP @Shear Rate 100000 1/s, Temperature 446 °F |
|
DSM Arnite® TV4 261 SF PBT-GF30 FR(17) 30% Glass Reinforced, Flame Retardant, High Flow |
|||
Viscosity | 20000 cP @Shear Rate 100000 1/s, Temperature 230 °C |
20000 cP @Shear Rate 100000 1/s, Temperature 446 °F |
|
DSM Arnite® TV4 441 (PBT+PET)-GF20 20% Glass Reinforced |
|||
Viscosity | 20000 cP @Shear Rate 100000 1/s, Temperature 230 °C |
20000 cP @Shear Rate 100000 1/s, Temperature 446 °F |
|
DSM Arnite® TV4 461 (PBT+PET)-GF30 30% Glass Reinforced |
|||
Viscosity | 20000 cP @Shear Rate 100000 1/s, Temperature 230 °C |
20000 cP @Shear Rate 100000 1/s, Temperature 446 °F |
|
DSM Arnite® TZ6 280 BLK (NCP-4718/B) PBT-(GF+GB)40 20% Glass Reinforced, 20% Glass Beads Reinforced |
|||
Viscosity | 20000 cP @Shear Rate 100000 1/s, Temperature 250 °C |
20000 cP @Shear Rate 100000 1/s, Temperature 482 °F |
|
DSM Arnite® TZ6 280 BLK (NCP-4718/B) PBT-(GF+GB)40 20% Glass Reinforced, 20% Glass Beads Reinforced |
|||
Viscosity | 20000 cP @Shear Rate 100000 1/s, Temperature 270 °C |
20000 cP @Shear Rate 100000 1/s, Temperature 518 °F |
|
DSM Arnite® TZ6 280 BLK (NCP-4718/B) PBT-(GF+GB)40 20% Glass Reinforced, 20% Glass Beads Reinforced |
|||
Viscosity | 20000 cP @Shear Rate 100000 1/s, Temperature 295 °C |
20000 cP @Shear Rate 100000 1/s, Temperature 563 °F |
|
DSM Arnite® AV2 390 XL PET GF50 50% Glass Reinforced, Low outgassing |
|||
Viscosity | 20000 - 40000 cP @Temperature 21.0 °C |
20000 - 40000 cP @Temperature 69.8 °F |
|
Abatron AboCast/AboCure 8109-11 All-purpose, structural dielectric resin. Better thermal and chemical properties than 8109-8, but requires heat cure. Melts at 70-80°C and remains liquid (supercooled) for many hours at RT.Process.. |
|||
Viscosity | 20000 cP @Frequency 10000 Hz, Temperature 277 °C |
20000 cP @Frequency 10000 Hz, Temperature 531 °F |
|
Akro-Plastic Akroloy® PA GF 50 (2706) PA 6.6 & PA6I/6T Dry, 50% Glass Filled One of the most characteristic properties of polyamide (PA 6.6) is the absorption of moisture. This essentially leads to increased toughness and elongation at break, to name the most important param.. |
|||
Viscosity | 20000 cP @Temperature 25.0 °C |
20000 cP @Temperature 77.0 °F |
|
Abatron AboCast 8708-10 One-Component Structural/Dielectric Epoxy AboCast 8708-10 is a highly filled, class H (180°C) structural, castable adhesive compound for FAST high-temperature curing. Suggested Uses: Structural bonding; Casting; Potting; Encapsulating; Em.. |
|||
Viscosity | 20000 cP @Temperature 25.0 °C |
20000 cP @Temperature 77.0 °F |
|
Abatron AboCast 8708-6 One-Component Structural/Dielectric Epoxy AboCast 8708-6 is a highly filled, class H (180°C) structural, castable adhesive compound for SLOW high-temperature curing. Suggested Uses: Structural bonding; Casting; Potting; Encapsulating; Emb.. |
|||
Viscosity | 20000 cP @Temperature 25.0 °C |
20000 cP @Temperature 77.0 °F |
|
Abatron AboCast 8708-9 One-Component Structural/Dielectric Epoxy AboCast 8708-9 is a highly filled, class H (180°C) structural, castable adhesive compound for FASTER high-temperature curing. Suggested Uses: Structural bonding; Casting; Potting; Encapsulating; E.. |
|||
Viscosity | 20000 cP @Shear Rate 100000 1/s, Temperature 230 °C |
20000 cP @Shear Rate 100000 1/s, Temperature 446 °F |
|
DSM Arnite® TZ6 280 PBT-(GF+GB)40 20% Glass Reinforced, 20% Glass Beads Reinforced |
|||
Viscosity | 20000 cP @Shear Rate 100000 1/s, Temperature 250 °C |
20000 cP @Shear Rate 100000 1/s, Temperature 482 °F |
|
DSM Arnite® TZ6 280 PBT-(GF+GB)40 20% Glass Reinforced, 20% Glass Beads Reinforced |
|||
Viscosity | 20000 cP @Shear Rate 100000 1/s, Temperature 270 °C |
20000 cP @Shear Rate 100000 1/s, Temperature 518 °F |
|
DSM Arnite® TZ6 280 PBT-(GF+GB)40 20% Glass Reinforced, 20% Glass Beads Reinforced |
|||
Viscosity | 20000 - 700000 cP @Temperature 230 - 270 °C |
20000 - 700000 cP @Temperature 446 - 518 °F |
Average value: 260000 cP Grade Count:2 |
Overview of materials for Polybutylene Terephthalate (PBT), Glass Bead Filled This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), Glass Bead Filled". Each property range of values reported is minimum .. |
|||
Viscosity | 20000 - 700000 cP @Shear Rate 1.00 - 100000 1/s |
20000 - 700000 cP @Shear Rate 1.00 - 100000 1/s |
Average value: 260000 cP Grade Count:2 |
Overview of materials for Polybutylene Terephthalate (PBT), Glass Bead Filled This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), Glass Bead Filled". Each property range of values reported is minimum .. |