Physical Properties | Metric | English | Comments |
---|---|---|---|
Viscosity | 2.26e+6 cP @Shear Rate 10.0 1/s, Temperature 190 °C |
2.26e+6 cP @Shear Rate 10.0 1/s, Temperature 374 °F |
10 rad/sec; ARES Rheometer |
Dow Engage® ENR 7256.00 Ethylene-Butene Copolymer Description: ENR 7256.00 is a unique broader molecular weight distribution ethylene-butene copolymer with higher branching levels that offers excellent clarity, processing and performance in foams a.. |