Physical Properties | Metric | English | Comments |
---|---|---|---|
Viscosity | 149600 cP @Shear Rate 500 1/s, Temperature 280 °C |
149600 cP @Shear Rate 500 1/s, Temperature 536 °F |
ISO 11403-1 -2 |
DuPont Performance Polymers Zytel® 7335F NC010 Nylon 6
(Unverified Data**) Unreinforced Polyamide 6 Zytel 7335F NC010 is a nucleated lubricated polyamide 6 resin for injection molding.Information provided by DuPont Performance Polymers |
|||
Viscosity | 149600 cP @Shear Rate 500 1/s, Temperature 280 °C |
149600 cP @Shear Rate 500 1/s, Temperature 536 °F |
ISO 11403-1 -2 |
DuPont Performance Polymers Zytel® 77G43L BK031 Nylon 612
(Unverified Data**) 43% Glass Reinforced Polyamide 612Information provided by DuPont Performance Polymers |