Physical Properties | Metric | English | Comments |
---|---|---|---|
Viscosity | 12500 cP @Shear Rate 100000 1/s, Temperature 270 °C |
12500 cP @Shear Rate 100000 1/s, Temperature 518 °F |
|
DSM Arnite® TV4 441 (PBT+PET)-GF20 20% Glass Reinforced |
|||
Viscosity | 12500 cP @Shear Rate 100000 1/s, Temperature 270 °C |
12500 cP @Shear Rate 100000 1/s, Temperature 518 °F |
|
DSM Arnite® TV4 461 (PBT+PET)-GF30 30% Glass Reinforced |
|||
Viscosity | 12500 cP @Shear Rate 100000 1/s, Temperature 310 °C |
12500 cP @Shear Rate 100000 1/s, Temperature 590 °F |
|
DSM Arnite® AV2 370 HF PET-GF35 35% Glass Reinforced, Brake Booster Body Valves, High Flow |
|||
Viscosity | 12500 cP @Shear Rate 100000 1/s, Temperature 270 °C |
12500 cP @Shear Rate 100000 1/s, Temperature 518 °F |
|
DSM Arnite® T06 202 /A PBT Medium Viscosity, Injection Molding |
|||
Viscosity | 12500 - 250000 cP @Temperature 270 - 310 °C |
12500 - 250000 cP @Temperature 518 - 590 °F |
Average value: 96700 cP Grade Count:1 |
Overview of materials for Polyethylene Terephthalate (PET), 40% Glass Reinforced This property data is a summary of similar materials in the MatWeb database for the category "Polyethylene Terephthalate (PET), 40% Glass Reinforced". Specific grades with glass content between 35% .. |
|||
Viscosity | 12500 - 250000 cP @Shear Rate 100 - 100000 1/s |
12500 - 250000 cP @Shear Rate 100 - 100000 1/s |
Average value: 96700 cP Grade Count:1 |
Overview of materials for Polyethylene Terephthalate (PET), 40% Glass Reinforced This property data is a summary of similar materials in the MatWeb database for the category "Polyethylene Terephthalate (PET), 40% Glass Reinforced". Specific grades with glass content between 35% .. |
|||
Viscosity | 12500 cP @Temperature 25.0 °C |
12500 cP @Temperature 77.0 °F |
|
Lendell Manufacturing Prepol Pre Polymer Liquid Apperance, Amber, honey likePolyether Polyurethane Pre-Polymer is water activated, yielding foams and gels with unique characteristics - Hydrophilic, Bio-Compatible, loading of additives to 8.. |