Physical Properties | Metric | English | Comments |
---|---|---|---|
Viscosity | 111000 cP @Shear Rate 5000 1/s, Temperature 230 °C |
111000 cP @Shear Rate 5000 1/s, Temperature 446 °F |
ISO 11403-1 -2 |
DuPont Performance Polymers Delrin® 100AL NC010 Acetal (POM)
(Unverified Data**) Lubricated High Viscosity Acetal Homopolymer with Low Wear and Low Friction Delrin 100AL NC010 an unreinforced high viscosity lubricated acetal homopolymer resin containing an advanced system of lub.. |
|||
Viscosity | 111000 cP @Shear Rate 5000 1/s, Temperature 200 °C |
111000 cP @Shear Rate 5000 1/s, Temperature 392 °F |
ISO 11403-1 -2 |
DuPont Performance Polymers Delrin® 577 BK000 Acetal (POM)
(Unverified Data**) 20% Glass Filled Medium Viscosity Acetal Homopolymer Delrin 577 BK000 is a medium viscosity acetal homopolymer containing 20% glass fiber filler with high stiffness low warpage and low creep for sup.. |
|||
Viscosity | 111000 cP @Shear Rate 5000 1/s, Temperature 230 °C |
111000 cP @Shear Rate 5000 1/s, Temperature 446 °F |
ISO 11403-1 -2 |
DuPont Performance Polymers Delrin® FG100AL NC010 Acetal (POM)
(Unverified Data**) Lubricated High Viscosity Acetal Homopolymer with Low Wear and Low Friction Developed for Food Contact Applications Delrin FG100AL is a high viscosity lubricated acetal homopolymer resin containing .. |
|||
Viscosity | 111000 cP @Shear Rate 5000 1/s, Temperature 230 °C |
111000 cP @Shear Rate 5000 1/s, Temperature 446 °F |
ISO 11403-1 -2 |
DuPont Performance Polymers Delrin® 100AF Acetal (POM)
(Unverified Data**) 20% Teflon® Fiber Filled High Viscosity Acetal Homopolymer with Low Wear and Low Friction Delrin 100AF is a high viscosity acetal homopolymer containing 20% Teflon PTFE fibers. It is designed for a.. |