Physical Properties | Metric | English | Comments |
---|---|---|---|
Viscosity | 1.56 cP @Temperature 80.0 °C |
1.56 cP @Temperature 176 °F |
|
LG Chemical Phenol Structure & Characteristics: C6H5OH. Phenol is a white crystalline solid with a distinct smellUses: Raw material of phenolic resins, dye stuffs, synthetic fibers, herbicides, photo material, aromati.. |
|||
Viscosity | 1.56 cP @Temperature 230 °C |
1.56 cP @Temperature 446 °F |
?=50 sec<sup>-1</sup> |
Gromax Evasin EV-3201V Ethylene-Vinyl Alcohol Copolymer Unmodified random Co-Polymer of [Ethylene-Vinyl alcohol], designed for therm-plastic processing into Sheets and Foils with high Oxygen and Aroma Barrier EffectInformation provided by Gromax Enterpri.. |