Physical Properties | Metric | English | Comments |
---|---|---|---|
Viscosity | 800000 - 800000 cP @Temperature 320 - 320 °C |
800000 - 800000 cP @Temperature 608 - 608 °F |
Average value: 800000 cP Grade Count:1 |
Overview of materials for Polycarbonate, Extruded This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, Extruded". Each property range of values reported is minimum and maximum values of approp.. |
|||
Viscosity | 800000 - 800000 cP @Shear Rate 25.0 - 25.0 1/s |
800000 - 800000 cP @Shear Rate 25.0 - 25.0 1/s |
Average value: 800000 cP Grade Count:1 |
Overview of materials for Polycarbonate, Extruded This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, Extruded". Each property range of values reported is minimum and maximum values of approp.. |