Physical Properties | Metric | English | Comments |
---|---|---|---|
Viscosity | 250000 - 250000 cP @Temperature 260 - 260 °C |
250000 - 250000 cP @Temperature 500 - 500 °F |
Average value: 250000 cP Grade Count:1 |
Overview of materials for Polycarbonate, 30% Glass Filled This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, 30% Glass Filled". Specific grades with glass content between 25% and 34% are included. E.. |
|||
Viscosity | 250000 - 250000 cP @Shear Rate 1000 - 1000 1/s |
250000 - 250000 cP @Shear Rate 1000 - 1000 1/s |
Average value: 250000 cP Grade Count:1 |
Overview of materials for Polycarbonate, 30% Glass Filled This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, 30% Glass Filled". Specific grades with glass content between 25% and 34% are included. E.. |
|||
Viscosity | 12500 - 250000 cP @Temperature 270 - 310 °C |
12500 - 250000 cP @Temperature 518 - 590 °F |
Average value: 96700 cP Grade Count:1 |
Overview of materials for Polyethylene Terephthalate (PET), 40% Glass Reinforced This property data is a summary of similar materials in the MatWeb database for the category "Polyethylene Terephthalate (PET), 40% Glass Reinforced". Specific grades with glass content between 35% .. |
|||
Viscosity | 12500 - 250000 cP @Shear Rate 100 - 100000 1/s |
12500 - 250000 cP @Shear Rate 100 - 100000 1/s |
Average value: 96700 cP Grade Count:1 |
Overview of materials for Polyethylene Terephthalate (PET), 40% Glass Reinforced This property data is a summary of similar materials in the MatWeb database for the category "Polyethylene Terephthalate (PET), 40% Glass Reinforced". Specific grades with glass content between 35% .. |