Physical Properties | Metric | English | Comments |
---|---|---|---|
Viscosity | 1.00e+6 - 2.00e+6 cP @Temperature 190 - 190 °C |
1.00e+6 - 2.00e+6 cP @Temperature 374 - 374 °F |
Average value: 1.24e+6 cP Grade Count:5 |
Overview of materials for Ethylene Vinyl Acetate Copolymer (EVA), Extrusion/Coating Grade This property data is a summary of similar materials in the MatWeb database for the category "Ethylene Vinyl Acetate Copolymer (EVA), Extrusion/Coating Grade". Each property range of values reported.. |
|||
Viscosity | 1.00e+6 - 2.00e+6 cP @Shear Rate 50.0 - 50.0 1/s |
1.00e+6 - 2.00e+6 cP @Shear Rate 50.0 - 50.0 1/s |
Average value: 1.24e+6 cP Grade Count:5 |
Overview of materials for Ethylene Vinyl Acetate Copolymer (EVA), Extrusion/Coating Grade This property data is a summary of similar materials in the MatWeb database for the category "Ethylene Vinyl Acetate Copolymer (EVA), Extrusion/Coating Grade". Each property range of values reported.. |
|||
Viscosity | 2.00e+6 - 2.00e+6 cP @Temperature 190 - 190 °C |
2.00e+6 - 2.00e+6 cP @Temperature 374 - 374 °F |
Average value: 2.00e+6 cP Grade Count:2 |
Overview of materials for Ethylene Vinyl Acetate Copolymer (EVA), Film Grade This property data is a summary of similar materials in the MatWeb database for the category "Ethylene Vinyl Acetate Copolymer (EVA), Film Grade". Each property range of values reported is minimum a.. |
|||
Viscosity | 2.00e+6 - 2.00e+6 cP @Shear Rate 50.0 - 50.0 1/s |
2.00e+6 - 2.00e+6 cP @Shear Rate 50.0 - 50.0 1/s |
Average value: 2.00e+6 cP Grade Count:2 |
Overview of materials for Ethylene Vinyl Acetate Copolymer (EVA), Film Grade This property data is a summary of similar materials in the MatWeb database for the category "Ethylene Vinyl Acetate Copolymer (EVA), Film Grade". Each property range of values reported is minimum a.. |
|||
Viscosity | 2.00e+6 - 2.00e+6 cP @Temperature 240 - 240 °C |
2.00e+6 - 2.00e+6 cP @Temperature 464 - 464 °F |
Average value: 2.00e+6 cP Grade Count:1 |
Overview of materials for Acrylic, Optical Grade, Molded This property data is a summary of similar materials in the MatWeb database for the category "Acrylic, Optical Grade, Molded". Each property range of values reported is minimum and maximum values of.. |
|||
Viscosity | 2.00e+6 - 2.00e+6 cP @Shear Rate 100 - 100 1/s |
2.00e+6 - 2.00e+6 cP @Shear Rate 100 - 100 1/s |
Average value: 2.00e+6 cP Grade Count:1 |
Overview of materials for Acrylic, Optical Grade, Molded This property data is a summary of similar materials in the MatWeb database for the category "Acrylic, Optical Grade, Molded". Each property range of values reported is minimum and maximum values of.. |