Physical Properties | Metric | English | Comments |
---|---|---|---|
Viscosity | 50400 cP @Shear Rate 5000 1/s, Temperature 300 °C |
50400 cP @Shear Rate 5000 1/s, Temperature 572 °F |
ISO 11403-1 -2 |
DuPont Performance Polymers Zytel® 77G43L BK031 Nylon 612
(Unverified Data**) 43% Glass Reinforced Polyamide 612Information provided by DuPont Performance Polymers |