Physical Properties | Metric | English | Comments |
---|---|---|---|
Viscosity | 500000 cP @Temperature 25.0 °C |
500000 cP @Temperature 77.0 °F |
ET536B, Polyamine Hardener |
Permabond ET536 Epoxy Resin PERMABOND ET536 is a two-part, 1:1 mixable epoxy adhesive with good adhesion to a variety of substrates such as wood, metal, ceramics and some plastics and composites. Permabond ET536 forms tough bo.. |
|||
Viscosity | 500000 cP @Temperature 25.0 °C |
500000 cP @Temperature 77.0 °F |
at 2rpm vibration |
Permabond HH167 Anaerobic Retainer Permabond® HH167 is a high viscosity gap filling silver paste, which can be used for repairing metal machinery parts. It is ideal for repairing worn shafts, broken threads, damaged keyways and spli.. |
|||
Viscosity | 500000 cP @Temperature 25.0 °C |
500000 cP @Temperature 77.0 °F |
at 2 rpm vibration |
Permabond MH196 Anaerobic Gasketmaker Permabond® MH196 is an anaerobic material designed for making “formed in situ” gaskets between metal surfaces. It is capable of replacing a wide range of conventional gaskets, thereby offering po.. |
|||
Viscosity | 500000 cP @Shear Rate 1.00 1/s, Temperature 250 °C |
500000 cP @Shear Rate 1.00 1/s, Temperature 482 °F |
|
DSM Arnite® TM4 440 (PBT+PET)-MD20 20% Mineral Reinforced |
|||
Viscosity | 500000 cP @Shear Rate 1.00 1/s, Temperature 250 °C |
500000 cP @Shear Rate 1.00 1/s, Temperature 482 °F |
|
DSM Arnite® TZ6 280 BLK (NCP-4718/B) PBT-(GF+GB)40 20% Glass Reinforced, 20% Glass Beads Reinforced |
|||
Viscosity | 500000 cP @Shear Rate 1.00 1/s, Temperature 250 °C |
500000 cP @Shear Rate 1.00 1/s, Temperature 482 °F |
|
DSM Arnite® T06 202 /A PBT Medium Viscosity, Injection Molding |
|||
Viscosity | 500000 cP @Shear Rate 1.00 1/s, Temperature 250 °C |
500000 cP @Shear Rate 1.00 1/s, Temperature 482 °F |
|
DSM Arnite® TZ6 280 PBT-(GF+GB)40 20% Glass Reinforced, 20% Glass Beads Reinforced |
|||
Viscosity | 500000 - 900000 cP @Temperature 190 - 190 °C |
500000 - 900000 cP @Temperature 374 - 374 °F |
Average value: 700000 cP Grade Count:3 |
Overview of materials for Ethylene-Methyl Acrylate Copolymer, Coating Grade This property data is a summary of similar materials in the MatWeb database for the category "Ethylene-Methyl Acrylate Copolymer, Coating Grade". Each property range of values reported is minimum an.. |
|||
Viscosity | 500000 - 900000 cP @Shear Rate 50.0 - 50.0 1/s |
500000 - 900000 cP @Shear Rate 50.0 - 50.0 1/s |
Average value: 700000 cP Grade Count:3 |
Overview of materials for Ethylene-Methyl Acrylate Copolymer, Coating Grade This property data is a summary of similar materials in the MatWeb database for the category "Ethylene-Methyl Acrylate Copolymer, Coating Grade". Each property range of values reported is minimum an.. |