Physical Properties | Metric | English | Comments |
---|---|---|---|
Viscosity | 267000 cP @Shear Rate 500 1/s, Temperature 230 °C |
267000 cP @Shear Rate 500 1/s, Temperature 446 °F |
ISO 11403-1 -2 |
DuPont Performance Polymers Hytrel® 4056 Polyester Elastomer TPC-ET
(Unverified Data**) 40 Shore D High Performance Polyester ElastomerInformation provided by DuPont Performance Polymers |