Physical Properties | Metric | English | Comments |
---|---|---|---|
Viscosity | 218000 cP @Shear Rate 500 1/s, Temperature 260 °C |
218000 cP @Shear Rate 500 1/s, Temperature 500 °F |
ISO 11403-1 -2 |
DuPont Performance Polymers Hytrel® 7246 Polyester Elastomer TPC-ET
(Unverified Data**) 72 Shore D High Performance Polyester Elastomer.Information provided by DuPont Performance Polymers |
|||
Viscosity | 218000 cP @Shear Rate 681 1/s, Temperature 305 °C |
218000 cP @Shear Rate 681 1/s, Temperature 581 °F |
ISO 11443 |
DuPont Performance Polymers Rynite® 408 NC010 PET Rynite® 408 NC010 is a 30% glass reinforced modified polyethylene terephthalate with improved impact resistance. Excellent balance of strength, stiffness, toughness, and temperature resistance.Inf.. |