Physical Properties | Metric | English | Comments |
---|---|---|---|
Viscosity | 20500 cP @Temperature 25.0 °C |
20500 cP @Temperature 77.0 °F |
at 20 rpm vibration |
Permabond LH197 Anaerobic Gasketmaker Permabond® LH197 is an anaerobic material designed for making “formed in situ” gaskets between metal surfaces. It is highly flexible, making it ideal for dissimilar surfaces where differential th.. |