Physical Properties | Metric | English | Comments |
---|---|---|---|
Viscosity | 203000 cP @Shear Rate 2000 1/s, Temperature 250 °C |
203000 cP @Shear Rate 2000 1/s, Temperature 482 °F |
ISO 11443 |
DuPont Performance Polymers Crastin® SK609 NC010 PBT
(Unverified Data**) Crastin® SK609 NC010 is a 50% glass fiber reinforced, lubricated polybutylene terephthalate resin for injection molding.Information provided by DuPont Performance Polymers |
|||
Viscosity | 203000 cP @Shear Rate 500 1/s, Temperature 230 °C |
203000 cP @Shear Rate 500 1/s, Temperature 446 °F |
ISO 11403-1 -2 |
DuPont Performance Polymers Hytrel® G4774 Polyester Elastomer TPC-ET
(Unverified Data**) 47 Shore D Standard Performance Polyester Elastomer with Heat Ageing ProtectionHytrel G4774 is a medium modulus grade with nominal hardness of 47D. It contains discoloring stabilizer. It can be proc.. |
|||
Viscosity | 203000 cP @Shear Rate 500 1/s, Temperature 295 °C |
203000 cP @Shear Rate 500 1/s, Temperature 563 °F |
ISO 11403-1 -2 |
DuPont Performance Polymers Rynite® 935 NC010 Polyethylene Terephthalate (PET)
(Unverified Data**) 35% Glass Reinforced Polyethylene Terephthalate Rynite 935 NC010 is a 35% mica/glass reinforced modified polyethylene terephthalate resin with exceptionally low warpage excellent electrical properti.. |