Physical Properties | Metric | English | Comments |
---|---|---|---|
Viscosity | 19 cP @Shear Rate 1000 1/s, Temperature 290 °C |
19 cP @Shear Rate 1000 1/s, Temperature 554 °F |
|
Solvay TECHNYL® A 221 PA66, DRY Description TECHNYL ® A 221 is an unreinforced polyamide 66, medium viscosity, for injection molding, with a special crystallizing agent, for fast cycles. It is available in natural colors. Benef.. |
|||
Viscosity | >= 19 cP @Time 3600 sec |
>= 19 cP @Time 1.00 hour |
V-135-1 |
Solvay JAGUAR® 413 Surfactant Description: Nonyl phenol based non ionic surfactant (70 EO)Chemical Name: GALACTOMANNAN BLENDCAS: 39421-75-5; 7631-86-9 Available in: Asia Pacific, Europe, Latin America and North AmericaApplicatio.. |
|||
Viscosity | >= 19 cP @Time 86400 sec |
>= 19 cP @Time 24.0 hour |
V-135-1 |
Solvay JAGUAR® 413 Surfactant Description: Nonyl phenol based non ionic surfactant (70 EO)Chemical Name: GALACTOMANNAN BLENDCAS: 39421-75-5; 7631-86-9 Available in: Asia Pacific, Europe, Latin America and North AmericaApplicatio.. |