Physical Properties | Metric | English | Comments |
---|---|---|---|
Viscosity | 12000 cP @Temperature 25.0 °C |
12000 cP @Temperature 77.0 °F |
ET500A, Epoxy Resin |
Permabond ET500 Epoxy Resin PERMABOND ET500 is a two-part fast-setting epoxy adhesive which bonds to a wide variety of substrates such as wood, metal, ceramics and some plastics and composites. It cures rapidly at room tempera.. |
|||
Viscosity | 12000 - 18000 cP @Shear Rate 50.0 1/s, Temperature 25.0 °C |
12000 - 18000 cP @Shear Rate 50.0 1/s, Temperature 77.0 °F |
Haake VT 550 PK1.1° |
Gwent Electronic Materials C2110309D5 Carbon Graphite Ink This is designed for screen-printing of working electrodes for electrochemical sensors. The paste is formulated to give superior printing properties with good definition for fine line printing.Produ.. |