Physical Properties | Metric | English | Comments |
---|---|---|---|
Viscosity | 1.13e+6 cP @Shear Rate 500 1/s, Temperature 240 °C |
1.13e+6 cP @Shear Rate 500 1/s, Temperature 464 °F |
ISO 11403-1 -2 |
DuPont Performance Polymers Crastin® BM6450XD BK560 Polybutylene Terephthalate (PBT)
(Unverified Data**)& Unreinforced Polybutylene Terephthalate Developed for Blow MoldingCrastin BM6450XD BK560 is an unreinforced supertough polybutylene terephthalate resin with very high viscosity for extrusion and blo.. |