Physical Properties | Metric | English | Comments |
---|---|---|---|
Kinematic Viscosity at 100°C (212°F) | 8.8 cSt | 8.8 cSt | Base Oil; ASTM D445 |
Nye Lubricants 716B (RL) Rheolube Grease Information provided by Nye Lubricants. |
|||
Kinematic Viscosity at 100°C (212°F) | 8.8 cSt | 8.8 cSt | |
ChevronTexaco Hydraulic Safety Fluid Texaco Hydraulic Safety Fluid is a fire-resistant fluid designed for use in high pressure hydraulic systems where the requirements for fire resistance, pump wear protection and viscosity are satisfi.. |
|||
Kinematic Viscosity at 100°C (212°F) | 8.8 cSt | 8.8 cSt | |
ConocoPhillips Hydroclear Diamond Class® 68 AW Turbine Oil Diamond Class AW Turbine Oil is a premium quality, rust and oxidation (R&O)-inhibited, antiwear turbine oil developed for use in geared and direct-drive gas turbines and steam turbines in severe ser.. |
|||
Kinematic Viscosity at 100°C (212°F) | 8.8 cSt | 8.8 cSt | |
ConocoPhillips Hydroclear® 2 Ultra-clean multi-purpose R&O Oil, AGMA Lubricant No. 2 Description: Conoco Hydroclear Ultra-Clean Multipurpose R&O Oil is a rust- and oxidation-inhibited industrial oil with ashless wear protection formulated from premium Conoco hydrocracked base stocks.. |
|||
Kinematic Viscosity at 100°C (212°F) | 8.8 cSt | 8.8 cSt | |
ConocoPhillips Hydroclear® 68 Multipurpose R&O Oil, AGMA Lubricant No. 2 Description: Conoco Hydroclear Multipurpose R&O Oil is a rust- and oxidationinhibited industrial oil with ashless wear protection formulated from premium Conoco hydrocracked base stocks. Hydroclear .. |
|||
Kinematic Viscosity at 100°C (212°F) | 8.8 cSt | 8.8 cSt | |
ConocoPhillips Hydroclear Diamond Class® 68 Turbine Oil Diamond Class Turbine Oil is a premium quality, rust and oxidation (R&O)-inhibited turbine oil developed for use in gas turbines and steam turbines in severe service. It is specially formulated to p.. |