Physical Properties | Metric | English | Comments |
---|---|---|---|
Kinematic Viscosity at 100°C (212°F) | 23.4 cSt | 23.4 cSt | |
ChevronTexaco 320 Honor Ashless AW Texaco Honor Ashless AW are circulating oils formulated from high quality base stocks and a carefully balanced, zinc-free additive package. These proved excellent protection against wear for long be.. |
|||
Kinematic Viscosity at 100°C (212°F) | 23.4 cSt | 23.4 cSt | ASTM D445 |
ChevronTexaco ISO 320 Machine Oil AW FeaturesChevron Machine Oils AW are premium quality lubricants.They provide excellent antiwear protection, oxidation and corrosion inhibition, and foam and aeration suppression.They are excellent mu.. |
|||
Kinematic Viscosity at 100°C (212°F) | 23.4 cSt | 23.4 cSt | Base Oil |
ConocoPhillips 1 Milube® Grease 2100 NLGI No. 1 Description: Conoco Milube Grease is a high-quality, extreme-pressure lithium 12-hydroxy grease with heavy base oil developed for use in heavily loaded industrial heavy-duty bearings characteristic .. |
|||
Kinematic Viscosity at 100°C (212°F) | 23.4 cSt | 23.4 cSt | Base Oil |
ConocoPhillips 1 Milube® Grease 2100T NLGI No. 1 Description: Conoco Milube Grease is a high-quality, extreme-pressure lithium 12-hydroxy grease with heavy base oil developed for use in heavily loaded industrial heavy-duty bearings characteristic .. |