Physical Properties | Metric | English | Comments |
---|---|---|---|
Kinematic Viscosity at 100°C (212°F) | 20.6 cSt | 20.6 cSt | ASTM D445 |
ExxonMobil Mobilgrease HTM Mobilgrease HTR, HTM, HTS and HTF are high performance Extreme Pressure greases with exceptional resistance to the water contamination conditions typical of steel mill, surface mining, and off-highw.. |
|||
Kinematic Viscosity at 100°C (212°F) | 20.6 cSt | 20.6 cSt | ASTM D445 |
ExxonMobil Mobilgrease HTM Mobilgrease HTR, HTM, HTS and HTF are high performance Extreme Pressure greases with exceptional resistance to the water contamination conditions typical of steel mill, surface mining, and off-highw.. |