Physical Properties | Metric | English | Comments |
---|---|---|---|
Kinematic Viscosity at 100°C (212°F) | 19.2 cSt | 19.2 cSt | |
ChevronTexaco 100 Aircraft Engine Oil Texaco Aircraft Engine Oils deliver value through:Use of high quality straight mineral oil with low volatilityRigid quality control through production in an ISO 9002 certified facilityProvide a stab.. |
|||
Kinematic Viscosity at 100°C (212°F) | 19.2 cSt | 19.2 cSt | ASTM D445 |
ChevronTexaco Aero 50/Grade 100 Engine Oil AD Uncompounded FeaturesChevron Aero Engine Oils Uncompounded are a blend of high quality base oil, with small amounts of viscosity modifier for improved fluidity at cold temperatures, antioxidant, and antifoam age.. |
|||
Kinematic Viscosity at 100°C (212°F) | 19.2 cSt | 19.2 cSt | ASTM D-445 |
ConocoPhillips ANDEROL® AA Cooker & Valve Oil, High Temperature Water Resistant Food Grade ISO 220 Description: ANDEROL PQ AA Cooker & Valve Oil is a white mineral oil based product that meets the former H-1 approval requirements of the USDA where incidental food contact can occur. PQ AA Cooker &.. |