Physical Properties | Metric | English | Comments |
---|---|---|---|
Kinematic Viscosity at 100°C (212°F) | 10.8 cSt | 10.8 cSt | Base Oil; ASTM D445 |
Nye Lubricants UniFlor 8961 (UF) Synthetic Oil Information provided by Nye Lubricants. |
|||
Kinematic Viscosity at 100°C (212°F) | 10.8 cSt | 10.8 cSt | Base Oil; ASTM D445 |
Nye Lubricants UniFlor 8961F (896-1) (UF) Synthetic Oil Information provided by Nye Lubricants. |
|||
Kinematic Viscosity at 100°C (212°F) | 10.8 cSt | 10.8 cSt | Base Oil; ASTM D445 |
Nye Lubricants UniFlor 8961R (UF) Synthetic Oil Information provided by Nye Lubricants. |
|||
Kinematic Viscosity at 100°C (212°F) | 10.8 cSt | 10.8 cSt | Base Oil; ASTM D445 |
Nye Lubricants UniFlor 8961UF (UF) Synthetic Oil Information provided by Nye Lubricants. |
|||
Kinematic Viscosity at 100°C (212°F) | 10.8 cSt | 10.8 cSt | |
ChevronTexaco Canopus® 100 Texaco Canopus oils deliver value through:High resistance to forming emulsions due to excellent water separating characteristics.Long lubricant life provided by outstanding stability.Good lubricant .. |
|||
Kinematic Viscosity at 100°C (212°F) | 10.8 cSt | 10.8 cSt | ASTM D445 |
ChevronTexaco ECO® SAE 10W-30 Motor Oil FeaturesChevron ECO Motor Oil is formulated to be an environmentally responsible engine lubricant.It uses the highest quality re-refined base oils and special additives to protect against high tempe.. |
|||
Kinematic Viscosity at 100°C (212°F) | 10.8 cSt | 10.8 cSt | |
ChevronTexaco Havoline® SAE 10W-30 Motor Oil All grades of Havoline Motor Oils are formulated with high quality base stocks, a shear-stable viscosity index improver, and contain detergent, dispersant, wear control, antioxidant, corrosion inhib.. |
|||
Kinematic Viscosity at 100°C (212°F) | 10.8 cSt | 10.8 cSt | ASTM D445 |
ChevronTexaco ISO 100 AIO FeaturesChevron AIO (Chevron Authentic Industrial Oils) provide rust protection, oxidation inhibition, and foam suppression.Chevron AIO are good quality lubricants for any application not requiring .. |
|||
Kinematic Viscosity at 100°C (212°F) | 10.8 cSt | 10.8 cSt | ASTM D445 |
ChevronTexaco ISO 100 Utility Oil HVI FeaturesChevron Utility Oil HVI is a high quality, high viscosity index uncompounded oil with excellent water separating characteristics.Chevron Utility Oil HVI possesses good natural thermal and ox.. |
|||
Kinematic Viscosity at 100°C (212°F) | 10.8 cSt | 10.8 cSt | ASTM D445 |
ChevronTexaco Regal® 100 R&O Texaco Regal R&O oils deliver value through:Prolonged oil service life — Excellent oxidation stability provided by the multi-component inhibitor system resists oil breakdown during exposure to high.. |
|||
Kinematic Viscosity at 100°C (212°F) | 10.8 cSt | 10.8 cSt | ASTM D445 |
ChevronTexaco Supreme SAE 10W-30 Motor Oil FeaturesChevron Supreme Motor Oils are premium quality automotive engine oils.Chevron Supreme Motor Oils SAE 5W-20, 5W-30, 10W-30, 10W-40, and 20W-50 are formulated with ISO-SYN™ base stocks, a she.. |
|||
Kinematic Viscosity at 100°C (212°F) | 10.8 cSt | 10.8 cSt | ASTM D445 |
ChevronTexaco Supreme SAE 10W-30 Synthetic Blend Motor Oil FeaturesChevron Supreme Synthetic Blend Motor Oil is premium quality automotive engine oil.It is formulated with a combination of synthetic and premium quality conventional base oils and specially s.. |
|||
Kinematic Viscosity at 100°C (212°F) | 10.8 cSt | 10.8 cSt | ASTM D445 |
ChevronTexaco Supreme SAE 5W-30 Motor Oil FeaturesChevron Supreme Motor Oils are premium quality automotive engine oils.Chevron Supreme Motor Oils SAE 5W-20, 5W-30, 10W-30, 10W-40, and 20W-50 are formulated with ISO-SYN™ base stocks, a she.. |
|||
Kinematic Viscosity at 100°C (212°F) | 10.8 cSt | 10.8 cSt | ASTM D445 |
ChevronTexaco Supreme SAE 5W-30 Synthetic Blend Motor Oil FeaturesChevron Supreme Synthetic Blend Motor Oil is premium quality automotive engine oil.It is formulated with a combination of synthetic and premium quality conventional base oils and specially s.. |
|||
Kinematic Viscosity at 100°C (212°F) | 10.8 cSt | 10.8 cSt | |
ConocoPhillips Conoco® El Mar® 2000 Oil SAE Grade 30 Conoco® El Mar 2000 is a high-quality, very low-ash, dispersant detergent gas engine oil designed for use in naturally aspirated and moderately turbocharged, low- to medium-speed 2-stroke cycle and.. |
|||
Kinematic Viscosity at 100°C (212°F) | 10.8 cSt | 10.8 cSt | |
ConocoPhillips Hydroclear® El Mar® Low Ash Heavy Duty SAE 30 Description: Conoco Hydroclear El Mar Low Ash Heavy Duty is a high-quality low ash natural gas engine oil formulated from exclusive Conoco hydrocracked base stock. Hydroclear El Mar Low Ash Heavy Du.. |
|||
Kinematic Viscosity at 100°C (212°F) | 10.8 cSt | 10.8 cSt | |
ChevronTexaco Havoline® SAE 5W-30 Motor Oil All grades of Havoline Motor Oils are formulated with high quality base stocks, a shear-stable viscosity index improver, and contain detergent, dispersant, wear control, antioxidant, corrosion inhib.. |