Physical Properties | Metric | English | Comments |
---|---|---|---|
Kinematic Viscosity at 100°C (212°F) | 9.8 cSt | 9.8 cSt | |
ConocoPhillips Syncon® 68 Synthetic R&O Oil Syncon R&O Oil is a premium quality, synthetic, rust and oxidation (R&O)-inhibited circulating oil developed for use in circulating systems, rotary air compressors, lightly loaded enclosed gear driv.. |
|||
Kinematic Viscosity at 100°C (212°F) | 9.8 cSt | 9.8 cSt | ASTM D445 |
ChevronTexaco Dura-Lith® NLGI 0 Grease EP FeaturesChevron Dura-Lith Greases EP are multipurpose extreme pressure greases.They are manufactured using selected highly refined medium viscosity index base oils, a lithium 12-hydroxystearate thic.. |
|||
Kinematic Viscosity at 100°C (212°F) | 9.8 cSt | 9.8 cSt | ASTM D445 |
ChevronTexaco Dura-Lith® NLGI 00 Grease EP FeaturesChevron Dura-Lith Greases EP are multipurpose extreme pressure greases.They are manufactured using selected highly refined medium viscosity index base oils, a lithium 12-hydroxystearate thic.. |
|||
Kinematic Viscosity at 100°C (212°F) | 9.8 cSt | 9.8 cSt | |
ConocoPhillips Hydroclear® Fluid Description: Conoco Hydroclear PowerTran Fluid, formulated from premium hydrocracked base stock, is a multipurpose fluid for farm equipment, off-highway machinery, and industrial tractors whose tran.. |