Physical Properties | Metric | English | Comments |
---|---|---|---|
Kinematic Viscosity at 100°C (212°F) | 9.7 cSt | 9.7 cSt | Base Oil; ASTM D445 |
Nye Lubricants 182 (SO) Synthetic Oil Information provided by Nye Lubricants. |
|||
Kinematic Viscosity at 100°C (212°F) | 9.7 cSt | 9.7 cSt | Base Oil; ASTM D445 |
Nye Lubricants 9704S Grease Information provided by Nye Lubricants. |
|||
Kinematic Viscosity at 100°C (212°F) | 9.7 cSt | 9.7 cSt | |
ConocoPhillips SynXPA® 100 R&O Oil Description: Conoco SynXPA R&O Oil lubricates stationary and portable rotary compressors, as well as reciprocating compressors that operate in severe service. It is useful in single- and double-acti.. |
|||
Kinematic Viscosity at 100°C (212°F) | 9.7 cSt | 9.7 cSt | |
ChevronTexaco 2190 T-EP Military Symbol Oil Texaco Military Symbol Oil 2190 T-EP delivers value through:Long lubricant life because of selected base stocks and additives.Extreme pressure characteristics that provide high film strength to prot.. |
|||
Kinematic Viscosity at 100°C (212°F) | 9.7 cSt | 9.7 cSt | |
ChevronTexaco Regal® Marine 77 Texaco Regal Marine 77 delivers value through:Long lubricant life because of selected base stocks and additivesExtreme pressure characteristics provide high film strength to protect gears and bearin.. |
|||
Kinematic Viscosity at 100°C (212°F) | 9.7 cSt | 9.7 cSt | ASTM D445 |
ChevronTexaco SYMBOL 2190 Turbine Oil TEP FeaturesChevron Turbine Oil Symbol 2190 TEP was developed primarily as a circulating system oil for marine gear turbine sets.Chevron Turbine Oil Symbol 2190 TEP provides mild extreme pressure protec.. |
|||
Kinematic Viscosity at 100°C (212°F) | 9.7 cSt | 9.7 cSt | ASTM D-445 |
ConocoPhillips ANDEROL® FGH 68 Synthetic Food Grade Hydraulic Fluid, ISO 68 Description: ANDEROL FGH Series Hydraulic Fluids are made from synthetic hydrocarbons (PAO) and special additive packages which allow them to meet the former H-1 approval requirements of the USDA wh.. |