Physical Properties | Metric | English | Comments |
---|---|---|---|
Kinematic Viscosity at 100°C (212°F) | 5.3 cSt | 5.3 cSt | Base Oil; ASTM D445 |
Nye Lubricants 757SSG (RL) Synthetic Oil Information provided by Nye Lubricants. |
|||
Kinematic Viscosity at 100°C (212°F) | 5.3 cSt | 5.3 cSt | Base Oil; ASTM D445 |
Nye Lubricants 786A (RL) Synthetic Oil Information provided by Nye Lubricants. |
|||
Kinematic Viscosity at 100°C (212°F) | 5.3 cSt | 5.3 cSt | ASTM D445 |
ExxonMobil Teresstic 32 TERESSTIC is the brand name for a line of long-service-life lubricating oils that have ranked for over five decades among the finest products of their kind. Continually improved over the years, TERE.. |
|||
Kinematic Viscosity at 100°C (212°F) | 5.3 cSt | 5.3 cSt | ASTM D445 |
ExxonMobil Teresstic GT 32 Teresstic GT is a high-quality turbine oil formulated to provide effective day-in and day-out performance of steam turbine and gas turbine electricity generators and mechanical drive systems. Teress.. |
|||
Kinematic Viscosity at 100°C (212°F) | 5.3 cSt | 5.3 cSt | ASTM D445 |
ExxonMobil Univis HVI 13 Exxon Univis HVI is a line of premium performance anti-wear hydraulic oils characterized by their unusually high viscosity indexes. They are engineered to maintain close viscosity control over wide .. |
|||
Kinematic Viscosity at 100°C (212°F) | 5.3 cSt | 5.3 cSt | ASTM D445 |
ExxonMobil Mobil Vaculine 1405 Mobil Vacuoline 1400 Series oils are extra high performance lubricants specifically designed to satisfy the requirements of machine tools that use one oil for both hydraulic systems and way lubricat.. |
|||
Kinematic Viscosity at 100°C (212°F) | 5.3 cSt | 5.3 cSt | ASTM D445 |
ExxonMobil Mobil Vaculine 1405 Mobil Vacuoline 1400 Series oils are extra high performance lubricants specifically designed to satisfy the requirements of machine tools that use one oil for both hydraulic systems and way lubricat.. |
|||
Kinematic Viscosity at 100°C (212°F) | 5.3 cSt | 5.3 cSt | |
ExxonMobil Mobil Vaprotec Light Mobil Vaprotec Light is an ISO Viscosity Grade 32, turbine-quality circulation oil containing anti-oxidants and defoamants. It is enhanced with a three-phase rust inhibitor to protect surfaces light.. |
|||
Kinematic Viscosity at 100°C (212°F) | 5.3 cSt | 5.3 cSt | ASTM D445 |
ExxonMobil Teresstic 32 TERESSTIC is the brand name for a line of long-service-life lubricating oils that have ranked for over five decades among the finest products of their kind. Continually improved over the years, TERE.. |
|||
Kinematic Viscosity at 100°C (212°F) | 5.3 cSt | 5.3 cSt | ASTM D445 |
ExxonMobil Teresstic GT 32 Teresstic GT is a high-quality turbine oil formulated to provide effective day-in and day-out performance of steam turbine and gas turbine electricity generators and mechanical drive systems. Teress.. |
|||
Kinematic Viscosity at 100°C (212°F) | 5.3 cSt | 5.3 cSt | ASTM D445 |
ExxonMobil Univis HVI 13 Exxon Univis HVI is a line of premium performance anti-wear hydraulic oils characterized by their unusually high viscosity indexes. They are engineered to maintain close viscosity control over wide .. |
|||
Kinematic Viscosity at 100°C (212°F) | 5.3 cSt | 5.3 cSt | |
ExxonMobil Mobil Vaprotec Light Mobil Vaprotec Light is an ISO Viscosity Grade 32, turbine-quality circulation oil containing anti-oxidants and defoamants. It is enhanced with a three-phase rust inhibitor to protect surfaces light.. |