Physical Properties | Metric | English | Comments |
---|---|---|---|
Kinematic Viscosity at 100°C (212°F) | 5.1 cSt | 5.1 cSt | Base Oil; ASTM D445 |
Nye Lubricants UniFlor 8120 (473) (UF) Synthetic Oil Information provided by Nye Lubricants. |
|||
Kinematic Viscosity at 100°C (212°F) | 5.1 cSt | 5.1 cSt | Base Oil; ASTM D445 |
Nye Lubricants UniFlor 8122 (UF) Synthetic Oil Information provided by Nye Lubricants. |
|||
Kinematic Viscosity at 100°C (212°F) | 5.1 cSt @Temperature 100 °C |
5.1 cSt @Temperature 212 °F |
ASTM D445 |
PolyOne Synplast™ DUP-E Di Undecyl Phthalate Linear C11 phthalate esterContains 0.10-0.15 wt% 1,1,3-Tris (2-methyl-4hydroxy-5-t-butyl phenyl) butane antioxidantInformation provided by PolyOne |
|||
Kinematic Viscosity at 100°C (212°F) | 5.1 cSt | 5.1 cSt | ASTM D445 |
ExxonMobil Mobil Aero HF Mobil Aero HFA, HF, and HFS are formulated for aircraft systems where use of hydrocarbon-based hydraulic fluids is required. They are low viscosity products, high VI (viscosity index) fluid with exc.. |
|||
Kinematic Viscosity at 100°C (212°F) | 5.1 cSt | 5.1 cSt | ASTM D445 |
ExxonMobil Mobil Aero HFA Mobil Aero HFA, HF, and HFS are formulated for aircraft systems where use of hydrocarbon-based hydraulic fluids is required. They are low viscosity products, high VI (viscosity index) fluid with exc.. |
|||
Kinematic Viscosity at 100°C (212°F) | 5.1 cSt | 5.1 cSt | ASTM D445 |
ExxonMobil Mobil Jet Oil II Mobil Jet Oil II is a high performance aircraft-type gas turbine lubricant formulated with a combination of a highly stable synthetic base fluid and a unique chemical additive package. The combina.. |
|||
Kinematic Viscosity at 100°C (212°F) | 5.1 cSt | 5.1 cSt | ASTM D445 |
ExxonMobil Mobiltherm 43 Mobiltherm 43 is a formulated paraffinic type fluid designed for closed heat transfer systems operating at higher bulk temperatures including demanding open systems. It has a high specific heat an.. |
|||
Kinematic Viscosity at 100°C (212°F) | 5.1 cSt | 5.1 cSt | |
ChevronTexaco 5606G Aircraft Hydraulic Oil Texaco Aircraft Hydraulic Oil 5606G delivers value through:Minimum viscosity change over a range of operating temperaturesLow pour point which permits operation at the lowest temperatures generally .. |
|||
Kinematic Viscosity at 100°C (212°F) | 5.1 cSt | 5.1 cSt | |
ChevronTexaco Rando® HDZ 22 Texaco Rando HDZ oils deliver value through:High oxidation stability — Longer service life than attainable with conventional lubricants used in high pressure service.Protection against rust and cor.. |
|||
Kinematic Viscosity at 100°C (212°F) | 5.1 cSt | 5.1 cSt | ASTM D445 |
ExxonMobil SpectraSyn™ 5 Polyalphaolefin (PAO) Fluid Product Description: SpectraSyn™ Low Viscosity Polyalphaolefin (PAO) basestocks feature low temperature properties, low volatility, and improved thermal stability. SpectraSyn™ Low Viscosity (PAO) .. |
|||
Kinematic Viscosity at 100°C (212°F) | 5.1 cSt | 5.1 cSt | ASTM D445 |
ExxonMobil Mobiltherm 43 Mobiltherm 43 is a formulated paraffinic type fluid designed for closed heat transfer systems operating at higher bulk temperatures including demanding open systems. It has a high specific heat an.. |
|||
Kinematic Viscosity at 100°C (212°F) | 5.1 cSt | 5.1 cSt | ASTM D445 |
ChevronTexaco Aviation G Hydraulic Fluid FeaturesChevron Aviation Hydraulic Fluids are both manufactured from specially selected, highly refined, low viscosity and low pour point petroleum base stocks. They both contain a superior, shear .. |
|||
Kinematic Viscosity at 100°C (212°F) | 5.1 cSt | 5.1 cSt | ASTM D445 |
ExxonMobil Mobil Pyrogard 53 Mobil Pyrogard 53 is a high performance phosphate ester synthetic fluid designed to replace petroleum-based oils in hydraulic applications where operating conditions preclude the use of combustible .. |
|||
Kinematic Viscosity at 100°C (212°F) | 5.1 cSt | 5.1 cSt | |
ConocoPhillips Hydroclear® XHP 2-Cycle Engine Oil Description: Conoco Hydroclear XHP 2-Cycle Engine Oil is made with an advanced, high-stability base oil and highly effective additives. This unique combination allows the product to meet full NMMA T.. |
|||
Kinematic Viscosity at 100°C (212°F) | 5.1 cSt | 5.1 cSt | ASTM D445 |
ExxonMobil Mobil Aero HF Mobil Aero HFA, HF, and HFS are formulated for aircraft systems where use of hydrocarbon-based hydraulic fluids is required. They are low viscosity products, high VI (viscosity index) fluid with exc.. |
|||
Kinematic Viscosity at 100°C (212°F) | 5.1 cSt | 5.1 cSt | ASTM D445 |
ExxonMobil Mobil Aero HFA Mobil Aero HFA, HF, and HFS are formulated for aircraft systems where use of hydrocarbon-based hydraulic fluids is required. They are low viscosity products, high VI (viscosity index) fluid with exc.. |
|||
Kinematic Viscosity at 100°C (212°F) | 5.1 cSt | 5.1 cSt | ASTM D445 |
ExxonMobil Mobil Jet Oil II Mobil Jet Oil II is a high performance aircraft-type gas turbine lubricant formulated with a combination of a highly stable synthetic base fluid and a unique chemical additive package. The combina.. |
|||
Kinematic Viscosity at 100°C (212°F) | 5.1 cSt | 5.1 cSt | ASTM D445 |
ExxonMobil Mobil Pyrogard 53 Mobil Pyrogard 53 is a high performance phosphate ester synthetic fluid designed to replace petroleum-based oils in hydraulic applications where operating conditions preclude the use of combustible .. |