Physical Properties | Metric | English | Comments |
---|---|---|---|
Kinematic Viscosity at 100°C (212°F) | 47 cSt | 47 cSt | Base Oil; ASTM D445 |
Nye Lubricants 573H-40 (NT) Synthetic Oil Information provided by Nye Lubricants. |
|||
Kinematic Viscosity at 100°C (212°F) | 47 cSt | 47 cSt | Base Oil; ASTM D445 |
Nye Lubricants NC-140 Grease Information provided by Nye Lubricants. |
|||
Kinematic Viscosity at 100°C (212°F) | 47 cSt | 47 cSt | Base Oil; ASTM D445 |
Nye Lubricants UniFlor 8620 (496A) (UF) Synthetic Oil Information provided by Nye Lubricants. |
|||
Kinematic Viscosity at 100°C (212°F) | 47 cSt | 47 cSt | Base Oil; ASTM D445 |
Nye Lubricants UniFlor 8622 (851) (UF) Synthetic Oil Information provided by Nye Lubricants. |
|||
Kinematic Viscosity at 100°C (212°F) | 47 cSt | 47 cSt | Base Oil; ASTM D445 |
Nye Lubricants UniFlor 8622R (851RP) (UF) Synthetic Oil Information provided by Nye Lubricants. |
|||
Kinematic Viscosity at 100°C (212°F) | 47 cSt | 47 cSt | Base Oil; ASTM D445 |
Nye Lubricants UniFlor 8623 (717C) (UF) Synthetic Oil Information provided by Nye Lubricants. |
|||
Kinematic Viscosity at 100°C (212°F) | 47 cSt | 47 cSt | Base Oil; ASTM D445 |
Nye Lubricants UniFlor 8623G (UF) Synthetic Oil Information provided by Nye Lubricants. |
|||
Kinematic Viscosity at 100°C (212°F) | 47 cSt | 47 cSt | ASTM D445 |
ExxonMobil Unirex PF 500 Formulated with perfluoropolyether that has been thickened with a non-organic polytetrafluoroethylene, UNIREX PF 500 is a long-life, severe-service grease for bearings, valves, seals and other appli.. |
|||
Kinematic Viscosity at 100°C (212°F) | 47 cSt | 47 cSt | |
ChevronTexaco Pinnacle® EP 460 Texaco Pinnacle EP oils deliver value through:Excellent thermal and oxidation stability — The synthetic hydrocarbon base oils used in these products provide outstanding stability resulting in longe.. |
|||
Kinematic Viscosity at 100°C (212°F) | 47 cSt | 47 cSt | ASTM D445 |
ChevronTexaco TEGRA® ISO 460 Synthetic Gear Lubricant FeaturesChevron Tegra Synthetic Gear Lubricants are superior quality industrial EP gear lubricants.The most advanced formulation has been selected to provide superior load carrying and antiwear prop.. |
|||
Kinematic Viscosity at 100°C (212°F) | 47 cSt | 47 cSt | ASTM D445 |
ExxonMobil Unirex PF 500 Formulated with perfluoropolyether that has been thickened with a non-organic polytetrafluoroethylene, UNIREX PF 500 is a long-life, severe-service grease for bearings, valves, seals and other appli.. |