Physical Properties | Metric | English | Comments |
---|---|---|---|
Kinematic Viscosity at 100°C (212°F) | 4.9 cSt | 4.9 cSt | ASTM D445 |
ChevronTexaco Elite-Cut® AD Metal Working Fluid FeaturesChevron -Cut Metalworking Fluids are a complete line of chlorinated cutting oils. The line consists of individual products with antiweld and lubricity properties to cover practically all met.. |
|||
Kinematic Viscosity at 100°C (212°F) | 4.9 cSt | 4.9 cSt | |
ConocoPhillips MV22 Super Hydraulic Oil Description: Conoco Super Hydraulic Oil is a high-quality antiwear hydraulic fluid formulated from premium Conoco hydrocracked base stocks to provide superior water separation, antiwear protection, .. |
|||
Kinematic Viscosity at 100°C (212°F) | 4.9 cSt | 4.9 cSt | ASTM D445 |
ChevronTexaco Bright-Cut® NL Metal Working Fluid FeaturesChevron Bright-Cut Metalworking Fluids are a complete line of chlorine-free cutting oils that offer benefits not found in conventional cutting oils.The unique synthetic antiweld components .. |