Physical Properties | Metric | English | Comments |
---|---|---|---|
Kinematic Viscosity at 100°C (212°F) | 4.7 cSt | 4.7 cSt | Base Oil; ASTM D445 |
Nye Lubricants 716R (RL) Rheolube Grease Information provided by Nye Lubricants. |
|||
Kinematic Viscosity at 100°C (212°F) | 4.7 cSt | 4.7 cSt | Base Oil; ASTM D445 |
Nye Lubricants UniFlor 8110 (UF) Synthetic Oil Information provided by Nye Lubricants. |
|||
Kinematic Viscosity at 100°C (212°F) | 4.7 cSt | 4.7 cSt | ASTM D445 |
ChevronTexaco 5R Neutral Oil FeaturesChevron Neutral Oils are all-hydroprocessed, highly refined API Group II paraffinic base stocks. Their extremely low sulfur, nitrogen, and aromatic content give them excellent thermal and o.. |
|||
Kinematic Viscosity at 100°C (212°F) | 4.7 cSt | 4.7 cSt | ASTM D445 |
ExxonMobil Synesstic™ 5 Synthetic Fluid Product Description: Synesstic™ Alkylated Naphthalene (AN) represent a unique class of API Group V category fluids. Synesstic™ AN products offer improved hydrolytic, thermal and oxidative stabilit.. |