Physical Properties | Metric | English | Comments |
---|---|---|---|
Kinematic Viscosity at 100°C (212°F) | 38.6 cSt | 38.6 cSt | Base Oil; ASTM D445 |
Nye Lubricants 788 (NG) Synthetic Oil Information provided by Nye Lubricants. |
|||
Kinematic Viscosity at 100°C (212°F) | 38.6 cSt | 38.6 cSt | ASTM D445 |
ExxonMobil 632 Mobil SHC 600 Series Mobil SHC 600 Series lubricants are supreme performance gear and bearing oils designed to provide outstanding service in terms of equipment protection, oil life and problem-free operation. They are .. |
|||
Kinematic Viscosity at 100°C (212°F) | 38.6 cSt | 38.6 cSt | ASTM D445 |
ExxonMobil 632 Mobil SHC 600 Series Mobil SHC 600 Series lubricants are supreme performance gear and bearing oils designed to provide outstanding service in terms of equipment protection, oil life and problem-free operation. They are .. |