Physical Properties | Metric | English | Comments |
---|---|---|---|
Kinematic Viscosity at 100°C (212°F) | 24.5 cSt | 24.5 cSt | ASTM D445 |
ExxonMobil 220 Mobil DTE FM Series Mobil DTE FM Series oils are high performance lubricants designed to satisfy a wide range of multi-use equipment requirements for the food processing and packaging industry. These lubricants are qua.. |
|||
Kinematic Viscosity at 100°C (212°F) | 24.5 cSt | 24.5 cSt | ASTM D445 |
ExxonMobil 632 Mobilgear 600 Series The Mobilgear 600 Series are extra high performance gear oils having outstanding extreme pressure characteristics and load-carrying properties, intended for use in all types of enclosed gear drives .. |
|||
Kinematic Viscosity at 100°C (212°F) | 24.5 cSt | 24.5 cSt | ASTM D445 |
ExxonMobil Spartan EP 320 Exxon SPARTAN EP lubricants are a family of premium quality extreme pressure gear lubricants. They are formulated with high quality mineral oils, which help reduce sludge formation and oil thickenin.. |
|||
Kinematic Viscosity at 100°C (212°F) | 24.5 cSt | 24.5 cSt | ASTM D445 |
ExxonMobil 220 Mobil DTE FM Series Mobil DTE FM Series oils are high performance lubricants designed to satisfy a wide range of multi-use equipment requirements for the food processing and packaging industry. These lubricants are qua.. |
|||
Kinematic Viscosity at 100°C (212°F) | 24.5 cSt | 24.5 cSt | ASTM D445 |
ExxonMobil 632 Mobilgear 600 Series The Mobilgear 600 Series are extra high performance gear oils having outstanding extreme pressure characteristics and load-carrying properties, intended for use in all types of enclosed gear drives .. |
|||
Kinematic Viscosity at 100°C (212°F) | 24.5 cSt | 24.5 cSt | ASTM D445 |
ExxonMobil Spartan EP 320 Exxon SPARTAN EP lubricants are a family of premium quality extreme pressure gear lubricants. They are formulated with high quality mineral oils, which help reduce sludge formation and oil thickenin.. |