Polymer Property : Kinematic Viscosity at 100°C (212°F) = 20.6 cSt Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Kinematic Viscosity at 100°C (212°F) 20.6 cSt
20.6 cSt
ASTM D445
ExxonMobil Mobilgrease HTM
Mobilgrease HTR, HTM, HTS and HTF are high performance Extreme Pressure greases with exceptional resistance to the water contamination conditions typical of steel mill, surface mining, and off-highw..
Kinematic Viscosity at 100°C (212°F) 20.6 cSt
20.6 cSt
ASTM D445
ExxonMobil Mobilgrease HTM
Mobilgrease HTR, HTM, HTS and HTF are high performance Extreme Pressure greases with exceptional resistance to the water contamination conditions typical of steel mill, surface mining, and off-highw..