Physical Properties | Metric | English | Comments |
---|---|---|---|
Kinematic Viscosity at 100°C (212°F) | 20 cSt | 20 cSt | Base Oil; ASTM D445 |
Nye Lubricants 231(SO) Synthetic Oil Information provided by Nye Lubricants. |
|||
Kinematic Viscosity at 100°C (212°F) | 20 cSt | 20 cSt | Base Oil; ASTM D445 |
Nye Lubricants 272 (SO) Synthetic Oil Information provided by Nye Lubricants. |
|||
Kinematic Viscosity at 100°C (212°F) | 20 cSt | 20 cSt | Base Oil; ASTM D445 |
Nye Lubricants 436 (SO) Synthetic Oil Information provided by Nye Lubricants. |
|||
Kinematic Viscosity at 100°C (212°F) | 20 cSt | 20 cSt | Base Oil; ASTM D445 |
Nye Lubricants 790G (RL) Synthetic Oil Information provided by Nye Lubricants. |
|||
Kinematic Viscosity at 100°C (212°F) | 20 cSt | 20 cSt | Base Oil; ASTM D445 |
Nye Lubricants 790G-MS (RL) Synthetic Oil Information provided by Nye Lubricants. |
|||
Kinematic Viscosity at 100°C (212°F) | 20 cSt | 20 cSt | Base Oil; ASTM D445 |
Nye Lubricants NYOSIL-M25 Oil Information provided by Nye Lubricants. |
|||
Kinematic Viscosity at 100°C (212°F) | 20 cSt | 20 cSt | Base Oil; ASTM D445 |
Nye Lubricants NYOSIL-M25UV Oil Information provided by Nye Lubricants. |
|||
Kinematic Viscosity at 100°C (212°F) | 20 cSt | 20 cSt | ASTM D-445 |
ConocoPhillips ANDEROL® FGC 150 Compressor Fluid, Synthetic Food Grade ISO 150 Description: ANDEROL FGC 150 Compressor Fluid is a synthetic hydrocarbon (PAO) based lubricant formulated with special additive packages that provide good thermal and oxidative stability to keep val.. |
|||
Kinematic Viscosity at 100°C (212°F) | 20 cSt | 20 cSt | |
ConocoPhillips Hydroclear® 220 TCS Slideway lubricant Description: Conoco Hydroclear® TCS Slideway Lubricant is a premium demulsible machine tool way lubricant formulated from premium Conoco hydrocracked base stocks. Hydroclear TCS Slideway Lubricant .. |