Physical Properties | Metric | English | Comments |
---|---|---|---|
Kinematic Viscosity at 100°C (212°F) | 17 cSt | 17 cSt | Base Oil; ASTM D445 |
Nye Lubricants FTL-9000 Grease Information provided by Nye Lubricants. |
|||
Kinematic Viscosity at 100°C (212°F) | 17 cSt | 17 cSt | ASTM D445 |
ExxonMobil 150 Mobil DTE FM Series Mobil DTE FM Series oils are high performance lubricants designed to satisfy a wide range of multi-use equipment requirements for the food processing and packaging industry. These lubricants are qua.. |
|||
Kinematic Viscosity at 100°C (212°F) | 17 cSt | 17 cSt | Base Oil |
ConocoPhillips SUPER-STA NLGI No. 1 Description: Conoco Super-STA and Super-STA M Greases are premium-quality, extreme-pressure (EP), multipurpose lithium greases recommended for lubrication of wheel bearings, chassis, ball joints, C... |
|||
Kinematic Viscosity at 100°C (212°F) | 17 cSt | 17 cSt | Base Oil |
ConocoPhillips SUPER-STA NLGI No. 2 Description: Conoco Super-STA and Super-STA M Greases are premium-quality, extreme-pressure (EP), multipurpose lithium greases recommended for lubrication of wheel bearings, chassis, ball joints, C... |
|||
Kinematic Viscosity at 100°C (212°F) | 17 cSt | 17 cSt | |
ConocoPhillips Syncon® 75W-90 HP Synthetic Gear Oil Description: Conoco Syncon HP Synthetic Gear Oil is recommended for conventional and limited-slip differentials, as well as some manual transmissions commonly found in passenger cars, race cars, tru.. |
|||
Kinematic Viscosity at 100°C (212°F) | 17 cSt | 17 cSt | |
ELM® 80W90 Multi-Purpose Biodegradable – Biobased Gear Lubricant Description: ELM 80W90 Multi-Purpose Gear Lubricant is a premium quality biodegradable gear lubricant formulated with the best optimized Biotechbased™ USA-grown natural seed oil that surpasses the .. |
|||
Kinematic Viscosity at 100°C (212°F) | 17 cSt | 17 cSt | ASTM D445 |
ExxonMobil 150 Mobil DTE FM Series Mobil DTE FM Series oils are high performance lubricants designed to satisfy a wide range of multi-use equipment requirements for the food processing and packaging industry. These lubricants are qua.. |
|||
Kinematic Viscosity at 100°C (212°F) | 17 cSt | 17 cSt | Base Oil |
ConocoPhillips EP Conolith® Grease NLGI NO. 0 Description: Conoco EP Conolith Grease is a high-quality, multipurpose, extreme pressure lithium grease recommended for heavy-duty, heavily loaded antifriction and plain bearings. It is ideal for th.. |
|||
Kinematic Viscosity at 100°C (212°F) | 17 cSt | 17 cSt | Base Oil |
ConocoPhillips EP Conolith® Grease NLGI NO. 00 Description: Conoco EP Conolith Grease is a high-quality, multipurpose, extreme pressure lithium grease recommended for heavy-duty, heavily loaded antifriction and plain bearings. It is ideal for th.. |
|||
Kinematic Viscosity at 100°C (212°F) | 17 cSt | 17 cSt | Base Oil |
ConocoPhillips EP Conolith® Grease NLGI NO. 000 Description: Conoco EP Conolith Grease is a high-quality, multipurpose, extreme pressure lithium grease recommended for heavy-duty, heavily loaded antifriction and plain bearings. It is ideal for th.. |
|||
Kinematic Viscosity at 100°C (212°F) | 17 cSt | 17 cSt | Base Oil |
ConocoPhillips EP Conolith® Grease NLGI NO. 1 Description: Conoco EP Conolith Grease is a high-quality, multipurpose, extreme pressure lithium grease recommended for heavy-duty, heavily loaded antifriction and plain bearings. It is ideal for th.. |
|||
Kinematic Viscosity at 100°C (212°F) | 17 cSt | 17 cSt | Base Oil |
ConocoPhillips EP Conolith® Grease NLGI NO. 2 Description: Conoco EP Conolith Grease is a high-quality, multipurpose, extreme pressure lithium grease recommended for heavy-duty, heavily loaded antifriction and plain bearings. It is ideal for th.. |
|||
Kinematic Viscosity at 100°C (212°F) | 17 cSt | 17 cSt | Base Oil |
ConocoPhillips SUPER-STA M NLGI No.0 Description: Conoco Super-STA and Super-STA M Greases are premium-quality, extreme-pressure (EP), multipurpose lithium greases recommended for lubrication of wheel bearings, chassis, ball joints, C... |
|||
Kinematic Viscosity at 100°C (212°F) | 17 cSt | 17 cSt | Base Oil |
ConocoPhillips SUPER-STA M NLGI No.2 Description: Conoco Super-STA and Super-STA M Greases are premium-quality, extreme-pressure (EP), multipurpose lithium greases recommended for lubrication of wheel bearings, chassis, ball joints, C... |
|||
Kinematic Viscosity at 100°C (212°F) | 17 cSt | 17 cSt | ASTM D445 |
ChevronTexaco Delo® Synthetic Grease SF FeaturesChevron Delo Synthetic Grease SF is a high performance grease specifically engineered for trailer wheel-ends operating in all conditions, even under the most extreme high and low temperature.. |
|||
Kinematic Viscosity at 100°C (212°F) | 17 cSt | 17 cSt | Base Oil |
ConocoPhillips SUPER-STA M NLGI No.1 Description: Conoco Super-STA and Super-STA M Greases are premium-quality, extreme-pressure (EP), multipurpose lithium greases recommended for lubrication of wheel bearings, chassis, ball joints, C... |