Physical Properties | Metric | English | Comments |
---|---|---|---|
Kinematic Viscosity at 40°C (104°F) | 685 cSt | 685 cSt | |
ConocoPhillips Syncon® 680 Synthetic EP Gear Oil, AGMA No. 8EP Description: Conoco Syncon Synthetic EP Gear Oil is a synthetic polyalphaolefin (PAO) lubricant for enclosed gear sets requiring extreme-pressure gear oils and operating at high temperatures. It is .. |
|||
Kinematic Viscosity at 40°C (104°F) | 685 cSt | 685 cSt | See Note 1. |
ChevronTexaco Hot Punch Compound H Texaco Hot Punch Compound H is a dark, semi-fluid calcium soap thickened grease designed for use as a die lubricant. It contains graphite and telc, which enhance its lubricity.Typical test data are .. |