Physical Properties | Metric | English | Comments |
---|---|---|---|
Kinematic Viscosity at 40°C (104°F) | 39 cSt | 39 cSt | Base Oil; ASTM D445 |
Nye Lubricants 609 (SO) Synthetic Oil Information provided by Nye Lubricants. |
|||
Kinematic Viscosity at 40°C (104°F) | 39 cSt | 39 cSt | Base Oil; ASTM D445 |
Nye Lubricants 951 (RL) Synthetic Oil Information provided by Nye Lubricants. |
|||
Kinematic Viscosity at 40°C (104°F) | 39 cSt | 39 cSt | Base Oil; ASTM D445 |
Nye Lubricants NPE-UC7 Oil Information provided by Nye Lubricants. |
|||
Kinematic Viscosity at 40°C (104°F) | 39 cSt | 39 cSt | |
ExxonMobil Kutwell 82 KUTWELL is the trademark for a line of two high-performance "soluble" cutting fluids for cooling and lubricating the tool and work in machining operations. The line includes one petroleum-base fluid.. |
|||
Kinematic Viscosity at 40°C (104°F) | 39 cSt | 39 cSt | ASTM D445 |
ExxonMobil Mobil Delvac Synthetic ATF Mobil Delvac Synthetic ATF is a synthetic fluid designed that meets the demanding requirements of modern heavy duty automatic transmissions. The synthetic baseoil composition enables excellent perf.. |
|||
Kinematic Viscosity at 40°C (104°F) | 39 cSt | 39 cSt | ASTM D445 |
ChevronTexaco 7R Unconventional Base Oil FeaturesChevron Unconventional Base Oils (UCBOs) are all hydroprocessed, highly refined paraffinic base oils of exceptional performance and purity.Relative to conventional hydroprocessed and solvent.. |
|||
Kinematic Viscosity at 40°C (104°F) | 39 cSt | 39 cSt | ASTM D-445 |
ConocoPhillips ANDEROL® 783-0 Series Synthetic Food Grade Greases, NLGI Grade 0 Description: ANDEROL 783 Series Greases are made from synthetic hydrocarbons (PAO) and an aluminum complex soap thickener, allowing for a wide range of operating temperatures. The 783 Series Greases.. |
|||
Kinematic Viscosity at 40°C (104°F) | 39 cSt | 39 cSt | ASTM D-445 |
ConocoPhillips ANDEROL® 783-00 Series Synthetic Food Grade Greases, NLGI Grade 00 Description: ANDEROL 783 Series Greases are made from synthetic hydrocarbons (PAO) and an aluminum complex soap thickener, allowing for a wide range of operating temperatures. The 783 Series Greases.. |
|||
Kinematic Viscosity at 40°C (104°F) | 39 cSt | 39 cSt | ASTM D-445 |
ConocoPhillips ANDEROL® 783-1 Series Synthetic Food Grade Greases, NLGI Grade 1 Description: ANDEROL 783 Series Greases are made from synthetic hydrocarbons (PAO) and an aluminum complex soap thickener, allowing for a wide range of operating temperatures. The 783 Series Greases.. |
|||
Kinematic Viscosity at 40°C (104°F) | 39 cSt | 39 cSt | |
ExxonMobil Kutwell 82 KUTWELL is the trademark for a line of two high-performance "soluble" cutting fluids for cooling and lubricating the tool and work in machining operations. The line includes one petroleum-base fluid.. |
|||
Kinematic Viscosity at 40°C (104°F) | 39 cSt | 39 cSt | |
ConocoPhillips HD Fleet™ 10W Engine Oil Description: Conoco HD Fleet Engine Oil is a high-quality, single-grade oil formulated from Conoco's premium hydrocracked base stock and unique additive technology. This oil is highly recommende.. |
|||
Kinematic Viscosity at 40°C (104°F) | 39 cSt | 39 cSt | ASTM D445 |
ExxonMobil Mobil Delvac Synthetic ATF Mobil Delvac Synthetic ATF is a synthetic fluid designed that meets the demanding requirements of modern heavy duty automatic transmissions. The synthetic baseoil composition enables excellent perf.. |