Physical Properties | Metric | English | Comments |
---|---|---|---|
Kinematic Viscosity at 40°C (104°F) | 333 cSt | 333 cSt | |
ChevronTexaco 120 Aircraft Engine Oils Texaco Aircraft Engine Oils deliver value through:Use of high quality straight mineral oil with low volatilityRigid quality control through production in an ISO 9002 certified facilityProvide a stab.. |
|||
Kinematic Viscosity at 40°C (104°F) | 333 cSt | 333 cSt | ASTM D445 |
ChevronTexaco Aero SAE 60/Grade 120 Engine Oil Uncompounded FeaturesChevron Aero Engine Oils Uncompounded are a blend of high quality base oil, with small amounts of viscosity modifier for improved fluidity at cold temperatures, antioxidant, and antifoam age.. |
|||
Kinematic Viscosity at 40°C (104°F) | 333 cSt | 333 cSt | ASTM D445 |
ExxonMobil HD Plus 85W-140 Mobilube HD Plus 80W-90 and 85W-140 are extra high performance commercial gear lubricants formulated from select base oils and an advanced additive system. These lubricants are engineered for perfor.. |
|||
Kinematic Viscosity at 40°C (104°F) | 333 cSt | 333 cSt | ASTM D445 |
ExxonMobil HD Plus 85W-140 Mobilube HD Plus 80W-90 and 85W-140 are extra high performance commercial gear lubricants formulated from select base oils and an advanced additive system. These lubricants are engineered for perfor.. |