Physical Properties | Metric | English | Comments |
---|---|---|---|
Kinematic Viscosity at 40°C (104°F) | 195 cSt | 195 cSt | ASTM D445 |
ExxonMobil 50 Mobiltrans HD Mobiltrans HD 10W, 30, 50, and 60 are extra high performance transmission and drive-train lubricants engineered to meet the rigorous specifications required by Caterpillar TO-4. This product line .. |
|||
Kinematic Viscosity at 40°C (104°F) | 195 cSt | 195 cSt | ASTM D445 |
ChevronTexaco Dura-Lith® NLGI 1 Grease EP FeaturesChevron Dura-Lith Greases EP are multipurpose extreme pressure greases.They are manufactured using selected highly refined medium viscosity index base oils, a lithium 12-hydroxystearate thic.. |
|||
Kinematic Viscosity at 40°C (104°F) | 195 cSt | 195 cSt | ASTM D445 |
ChevronTexaco Dura-Lith® NLGI 2 Grease EP FeaturesChevron Dura-Lith Greases EP are multipurpose extreme pressure greases.They are manufactured using selected highly refined medium viscosity index base oils, a lithium 12-hydroxystearate thic.. |
|||
Kinematic Viscosity at 40°C (104°F) | 195 cSt | 195 cSt | ASTM D445 |
ChevronTexaco Dura-Lith® NLGI 3 Grease EP FeaturesChevron Dura-Lith Greases EP are multipurpose extreme pressure greases.They are manufactured using selected highly refined medium viscosity index base oils, a lithium 12-hydroxystearate thic.. |
|||
Kinematic Viscosity at 40°C (104°F) | 195 cSt | 195 cSt | ASTM D445 |
ExxonMobil 50 Mobiltrans HD Mobiltrans HD 10W, 30, 50, and 60 are extra high performance transmission and drive-train lubricants engineered to meet the rigorous specifications required by Caterpillar TO-4. This product line .. |