Physical Properties | Metric | English | Comments |
---|---|---|---|
Kinematic Viscosity at 40°C (104°F) | 190 cSt | 190 cSt | Base Oil |
ConocoPhillips SUPER-STA NLGI No. 1 Description: Conoco Super-STA and Super-STA M Greases are premium-quality, extreme-pressure (EP), multipurpose lithium greases recommended for lubrication of wheel bearings, chassis, ball joints, C... |
|||
Kinematic Viscosity at 40°C (104°F) | 190 cSt | 190 cSt | Base Oil |
ConocoPhillips SUPER-STA NLGI No. 2 Description: Conoco Super-STA and Super-STA M Greases are premium-quality, extreme-pressure (EP), multipurpose lithium greases recommended for lubrication of wheel bearings, chassis, ball joints, C... |
|||
Kinematic Viscosity at 40°C (104°F) | 190 cSt | 190 cSt | Base Oil |
ConocoPhillips EP Conolith® Grease NLGI NO. 0 Description: Conoco EP Conolith Grease is a high-quality, multipurpose, extreme pressure lithium grease recommended for heavy-duty, heavily loaded antifriction and plain bearings. It is ideal for th.. |
|||
Kinematic Viscosity at 40°C (104°F) | 190 cSt | 190 cSt | Base Oil |
ConocoPhillips EP Conolith® Grease NLGI NO. 00 Description: Conoco EP Conolith Grease is a high-quality, multipurpose, extreme pressure lithium grease recommended for heavy-duty, heavily loaded antifriction and plain bearings. It is ideal for th.. |
|||
Kinematic Viscosity at 40°C (104°F) | 190 cSt | 190 cSt | Base Oil |
ConocoPhillips EP Conolith® Grease NLGI NO. 000 Description: Conoco EP Conolith Grease is a high-quality, multipurpose, extreme pressure lithium grease recommended for heavy-duty, heavily loaded antifriction and plain bearings. It is ideal for th.. |
|||
Kinematic Viscosity at 40°C (104°F) | 190 cSt | 190 cSt | Base Oil |
ConocoPhillips EP Conolith® Grease NLGI NO. 1 Description: Conoco EP Conolith Grease is a high-quality, multipurpose, extreme pressure lithium grease recommended for heavy-duty, heavily loaded antifriction and plain bearings. It is ideal for th.. |
|||
Kinematic Viscosity at 40°C (104°F) | 190 cSt | 190 cSt | Base Oil |
ConocoPhillips EP Conolith® Grease NLGI NO. 2 Description: Conoco EP Conolith Grease is a high-quality, multipurpose, extreme pressure lithium grease recommended for heavy-duty, heavily loaded antifriction and plain bearings. It is ideal for th.. |
|||
Kinematic Viscosity at 40°C (104°F) | 190 cSt | 190 cSt | Base Oil |
ConocoPhillips SUPER-STA M NLGI No.0 Description: Conoco Super-STA and Super-STA M Greases are premium-quality, extreme-pressure (EP), multipurpose lithium greases recommended for lubrication of wheel bearings, chassis, ball joints, C... |
|||
Kinematic Viscosity at 40°C (104°F) | 190 cSt | 190 cSt | Base Oil |
ConocoPhillips SUPER-STA M NLGI No.2 Description: Conoco Super-STA and Super-STA M Greases are premium-quality, extreme-pressure (EP), multipurpose lithium greases recommended for lubrication of wheel bearings, chassis, ball joints, C... |
|||
Kinematic Viscosity at 40°C (104°F) | 190 cSt | 190 cSt | Base Oil |
ConocoPhillips SUPER-STA M NLGI No.1 Description: Conoco Super-STA and Super-STA M Greases are premium-quality, extreme-pressure (EP), multipurpose lithium greases recommended for lubrication of wheel bearings, chassis, ball joints, C... |