Physical Properties | Metric | English | Comments |
---|---|---|---|
Kinematic Viscosity at 40°C (104°F) | 15.8 cSt | 15.8 cSt | ASTM D445 |
ChevronTexaco 8-T White Oil FeaturesChevron White Oils are technical grade oils processed from paraffinic oil. Mixtures of paraffinic and naphthenic hydrocarbons, they are virtually free of nitrogen, sulfur, oxygen, and aroma.. |
|||
Kinematic Viscosity at 40°C (104°F) | 15.8 cSt | 15.8 cSt | ASTM D445 |
ChevronTexaco Mechanism LPS® ISO 15 Hydraulic Oil Chevron Mechanism LPS Hydraulic Oils are highly refined, paraffinic oils containing oxidation and rust inhibitors, and special antiwear additives to extend the life of hydraulic pumps and motor part.. |
|||
Kinematic Viscosity at 40°C (104°F) | 15.8 cSt | 15.8 cSt | ASTM D445 |
ChevronTexaco Packers Oil |
|||
Kinematic Viscosity at 40°C (104°F) | 15.8 cSt | 15.8 cSt | |
ChevronTexaco Rando® HDZ 15 Texaco Rando HDZ oils deliver value through:High oxidation stability — Longer service life than attainable with conventional lubricants used in high pressure service.Protection against rust and cor.. |
|||
Kinematic Viscosity at 40°C (104°F) | 15.8 cSt | 15.8 cSt | ASTM D445 |
ChevronTexaco Rykon® ISO 15 Premium Oil FeaturesChevron Rykon Premium Oils are designed to give maximum protection to hydraulic pumps.They are formulated with ISOSYN® base stocks incorporating antiwear additives, oxidation and corrosion .. |