Physical Properties | Metric | English | Comments |
---|---|---|---|
Kinematic Viscosity at 40°C (104°F) | 14.2 cSt @Temperature 40.0 °C |
14.2 cSt @Temperature 104 °F |
ASTM D445 |
PolyOne Synplast™ DIDA-E Di Isodecyl Adipate Branched C10 adipate esterContains 0.10-0.15 wt% 1,1,3-Tris (2-methyl-4hydroxy-5-t-butyl phenyl) butane antioxidantInformation provided by PolyOne |
|||
Kinematic Viscosity at 40°C (104°F) | 14.2 cSt | 14.2 cSt | ASTM D445 |
ExxonMobil Mobil Aero HFS Mobil Aero HFA, HF, and HFS are formulated for aircraft systems where use of hydrocarbon-based hydraulic fluids is required. They are low viscosity products, high VI (viscosity index) fluid with exc.. |
|||
Kinematic Viscosity at 40°C (104°F) | 14.2 cSt | 14.2 cSt | ASTM D445 |
ExxonMobil Mobil Aero HFS Mobil Aero HFA, HF, and HFS are formulated for aircraft systems where use of hydrocarbon-based hydraulic fluids is required. They are low viscosity products, high VI (viscosity index) fluid with exc.. |