Physical Properties | Metric | English | Comments |
---|---|---|---|
Kinematic Viscosity at 40°C (104°F) | 13.3 cSt | 13.3 cSt | |
ExxonMobil Mobil Avrex S Turbo 256 Mobil Avrex S Turbo 256 gas turbine lubricant is a combination of a highly stable synthetic base fluid and a unique chemical additive package. The combination provides outstanding thermal and oxid.. |
|||
Kinematic Viscosity at 40°C (104°F) | 13.3 cSt | 13.3 cSt | ASTM D445 |
ChevronTexaco Superla® 7 White Oil FeaturesChevron Superla White Oils are colorless, odorless, tasteless mixtures of saturated paraffinic and naphthenic hydrocarbons that span a viscosity range of 50-625 SUS at 100°F.These nearly ch.. |
|||
Kinematic Viscosity at 40°C (104°F) | 13.3 cSt | 13.3 cSt | |
ExxonMobil Mobil Avrex S Turbo 256 Mobil Avrex S Turbo 256 gas turbine lubricant is a combination of a highly stable synthetic base fluid and a unique chemical additive package. The combination provides outstanding thermal and oxid.. |
|||
Kinematic Viscosity at 40°C (104°F) | 13.3 cSt | 13.3 cSt | ASTM D445 |
ExxonMobil Socony Oven Conveyor Lubricant Socony Oven Conveyer Lubricant is a high performance product designed specifically for the lubrication of oven conveyor chains at temperatures up to 200 degrees celsius. It is formulated from a low .. |
|||
Kinematic Viscosity at 40°C (104°F) | 13.3 cSt | 13.3 cSt | ASTM D445 |
ExxonMobil Socony Oven Conveyor Lubricant Socony Oven Conveyer Lubricant is a high performance product designed specifically for the lubrication of oven conveyor chains at temperatures up to 200 degrees celsius. It is formulated from a low .. |