Physical Properties | Metric | English | Comments |
---|---|---|---|
Kinematic Viscosity at 40°C (104°F) | 460 cSt | 460 cSt | ASTM D445 |
ExxonMobil 1 Mobiltemp Series Mobiltemp Series greases are high performance clay-thickened products designed for the lubrication of plain and antifriction bearings operating at low speed and high temperature or under cycling con.. |
|||
Kinematic Viscosity at 40°C (104°F) | 460 cSt | 460 cSt | ASTM D445 |
ExxonMobil 2 Mobiltemp Series Mobiltemp Series greases are high performance clay-thickened products designed for the lubrication of plain and antifriction bearings operating at low speed and high temperature or under cycling con.. |
|||
Kinematic Viscosity at 40°C (104°F) | 460 cSt | 460 cSt | ASTM D445 |
ExxonMobil 2 Ronex Extra Duty Exxon RONEX Extra Duty is the brand name for a line of super premium quality high base oil viscosity greases designed for a wide range of heavy duty industrial and commercial vehicle applications Th.. |
|||
Kinematic Viscosity at 40°C (104°F) | 460 cSt | 460 cSt | ASTM D445 |
ExxonMobil 78 Mobiltemp Series Mobiltemp Series greases are high performance clay-thickened products designed for the lubrication of plain and antifriction bearings operating at low speed and high temperature or under cycling con.. |
|||
Kinematic Viscosity at 40°C (104°F) | 460 cSt | 460 cSt | ASTM D445 |
ExxonMobil Enmist EP 460 Esso ENMIST EP is a family of premium quality industrial lubricants designed for the oil-fog or mist-lubrication of machine components such as slideways, bearings, gears, chains etc. ENMIST EP mist .. |
|||
Kinematic Viscosity at 40°C (104°F) | 460 cSt | 460 cSt | ASTM D445 |
ExxonMobil Mobil Glygoyle 460 Mobil Glygoyle Series lubricants are supreme performance gear, bearing and compressor oils designed to provide outstanding benefits in terms of efficiency, long oil life, and equipment protection. T.. |
|||
Kinematic Viscosity at 40°C (104°F) | 460 cSt | 460 cSt | ASTM D445 |
ExxonMobil Teresstic 460 TERESSTIC is the brand name for a line of long-service-life lubricating oils that have ranked for over five decades among the finest products of their kind. Continually improved over the years, TERE.. |
|||
Kinematic Viscosity at 40°C (104°F) | 460 cSt | 460 cSt | ASTM D445 |
ExxonMobil 460 Mobilgear SHC Series The Mobilgear SHC Series lubricants are heavy-duty gear oils primarily designed for all kinds of enclosed gearing as well as plain and rolling element bearings. They are formulated from wax-free pol.. |
|||
Kinematic Viscosity at 40°C (104°F) | 460 cSt | 460 cSt | ASTM D445 |
ExxonMobil 460 Mobilith SHC PM Mobilith SHC PM greases are supreme performance products designed specifically for severe paper machine applications, including extreme temperature environments and exposure to different qualities o.. |
|||
Kinematic Viscosity at 40°C (104°F) | 460 cSt | 460 cSt | ASTM D445 |
ExxonMobil 460 Mobilith SHC Series Mobilith SHC Series greases are supreme performance products designed for a wide variety of applications at extremes of temperature. They combine the unique features of synthetic base fluids with th.. |
|||
Kinematic Viscosity at 40°C (104°F) | 460 cSt | 460 cSt | ASTM D445 |
ExxonMobil Mobil Vaculine 146 The Mobil Vacuoline 100 range is a series of extra high quality circulating system oils primarily intended for the lubrication of plain bearings in systems designed for full fluid lubrication, parti.. |
|||
Kinematic Viscosity at 40°C (104°F) | 460 cSt | 460 cSt | ASTM D445 |
ChevronTexaco ISO 460 Synthetic Wheel Motor Lubricant EP FeaturesChevron Synthetic Wheel Motor Lubricants EP are superior quality industrial EP gear lubricants. Their advanced formulation provides superior load carrying and antiwear properties; protection.. |
|||
Kinematic Viscosity at 40°C (104°F) | 460 cSt | 460 cSt | See Note 3. |
ChevronTexaco Polystar® Synthetic 4602 NLGI Grade Texaco Polystar Synthetic 4602 delivers value through:Wide application range — Suitable for high rpm operation, operating temperatures ranging from -40°C to 230°C (-40°F to 446°F) and offers ex.. |
|||
Kinematic Viscosity at 40°C (104°F) | 460 cSt | 460 cSt | ASTM D445 |
ChevronTexaco Regal® 460 Texaco Regal oil delivers value through:Long lubricant life provided by good natural thermal and oxidation stability.Good demulsibility, which assures good lubricant, film strength and reduced wear .. |
|||
Kinematic Viscosity at 40°C (104°F) | 460 cSt | 460 cSt | ASTM D445 |
ChevronTexaco Regal® 460 R&O Texaco Regal R&O oils deliver value through:Prolonged oil service life — Excellent oxidation stability provided by the multi-component inhibitor system resists oil breakdown during exposure to high.. |
|||
Kinematic Viscosity at 40°C (104°F) | 460 cSt | 460 cSt | ASTM D445 |
ExxonMobil 1 Mobiltemp Series Mobiltemp Series greases are high performance clay-thickened products designed for the lubrication of plain and antifriction bearings operating at low speed and high temperature or under cycling con.. |
|||
Kinematic Viscosity at 40°C (104°F) | 460 cSt | 460 cSt | ASTM D445 |
ExxonMobil 2 Mobiltemp Series Mobiltemp Series greases are high performance clay-thickened products designed for the lubrication of plain and antifriction bearings operating at low speed and high temperature or under cycling con.. |
|||
Kinematic Viscosity at 40°C (104°F) | 460 cSt | 460 cSt | ASTM D445 |
ExxonMobil 2 Moly Ronex Extra Duty Exxon RONEX Extra Duty is the brand name for a line of super premium quality high base oil viscosity greases designed for a wide range of heavy duty industrial and commercial vehicle applications Th.. |
|||
Kinematic Viscosity at 40°C (104°F) | 460 cSt | 460 cSt | ASTM D445 |
ExxonMobil 460 Mobilith SHC PM Mobilith SHC PM greases are supreme performance products designed specifically for severe paper machine applications, including extreme temperature environments and exposure to different qualities o.. |
|||
Kinematic Viscosity at 40°C (104°F) | 460 cSt | 460 cSt | ASTM D445 |
ExxonMobil 634 Mobilgear 600 Series The Mobilgear 600 Series are extra high performance gear oils having outstanding extreme pressure characteristics and load-carrying properties, intended for use in all types of enclosed gear drives .. |
|||
Kinematic Viscosity at 40°C (104°F) | 460 cSt | 460 cSt | ASTM D445 |
ExxonMobil 7 Mobilith SHC Series Mobilith SHC Series greases are supreme performance products designed for a wide variety of applications at extremes of temperature. They combine the unique features of synthetic base fluids with th.. |
|||
Kinematic Viscosity at 40°C (104°F) | 460 cSt | 460 cSt | ASTM D445 |
ExxonMobil Enmist EP 460 Esso ENMIST EP is a family of premium quality industrial lubricants designed for the oil-fog or mist-lubrication of machine components such as slideways, bearings, gears, chains etc. ENMIST EP mist .. |
|||
Kinematic Viscosity at 40°C (104°F) | 460 cSt | 460 cSt | ASTM D445 |
ExxonMobil Mobil Glygoyle 460 Mobil Glygoyle Series lubricants are supreme performance gear, bearing and compressor oils designed to provide outstanding benefits in terms of efficiency, long oil life, and equipment protection. T.. |
|||
Kinematic Viscosity at 40°C (104°F) | 460 cSt | 460 cSt | ASTM D445 |
ExxonMobil Mobil Vaculine 146 The Mobil Vacuoline 100 range is a series of extra high quality circulating system oils primarily intended for the lubrication of plain bearings in systems designed for full fluid lubrication, parti.. |
|||
Kinematic Viscosity at 40°C (104°F) | 460 cSt | 460 cSt | ASTM D445 |
ExxonMobil 600 W Super Mobil Cylinder Oil Mobil Cylinder oils are extra high performance high viscosity oils designed for use in enclosed worm gears operating at moderate to high speeds and temperatures, and where heavy loads, slow speeds o.. |
|||
Kinematic Viscosity at 40°C (104°F) | 460 cSt | 460 cSt | Base Oil |
ConocoPhillips 2 Bentone Grease NLGI No. 2 Description: Conoco Bentone Grease is a high-quality, smooth-textured, clay based grease developed for heavy-duty industrial machinery operating at very high temperatures. Unlike conventional soap-b.. |
|||
Kinematic Viscosity at 40°C (104°F) | 460 cSt | 460 cSt | Base Oil; ASTM D445 |
Nye Lubricants 865 (FG) Synthetic Oil Information provided by Nye Lubricants. |
|||
Kinematic Viscosity at 40°C (104°F) | 460 cSt | 460 cSt | ASTM D445 |
ExxonMobil 460 Mobilith SHC Series Mobilith SHC Series greases are supreme performance products designed for a wide variety of applications at extremes of temperature. They combine the unique features of synthetic base fluids with th.. |
|||
Kinematic Viscosity at 40°C (104°F) | 460 cSt | 460 cSt | ASTM D445 |
ExxonMobil 460 Special Mobiltemp SHC Series Mobiltemp SHC Series products are supreme performance antiwear greases primarily intended for high temperature applications. They combine the unique features of polyalphaolefin (PAO) synthetic base .. |
|||
Kinematic Viscosity at 40°C (104°F) | 460 cSt | 460 cSt | ASTM D445 |
ExxonMobil 461 Mobilgrease XHP Series Mobilgrease XHP Series products are extra high performance lithium complex greases intended for a wide variety of applications and severe operating conditions. These greases were designed to outper.. |