Physical Properties | Metric | English | Comments |
---|---|---|---|
Kinematic Viscosity at 40°C (104°F) | 45 cSt | 45 cSt | Base Oil; ASTM D445 |
Nye Lubricants 377AL (RL) Synthetic Oil Information provided by Nye Lubricants. |
|||
Kinematic Viscosity at 40°C (104°F) | 45 cSt @Temperature 40.0 °C |
45 cSt @Temperature 104 °F |
ASTM D445 |
PolyOne Synplast™ NOTM-E Tri (n-octyl) Trimellitate Linear trimellitate esterContains 0.10-0.15 wt% 1,1,3-Tris (2-methyl-4hydroxy-5-t-butyl phenyl) butane antioxidantInformation provided by PolyOne |
|||
Kinematic Viscosity at 40°C (104°F) | 45 cSt @Temperature 40.0 °C |
45 cSt @Temperature 104 °F |
ASTM D445 |
PolyOne Synplast™ NOTM-PPC Tri (n-octyl) Trimellitate CPSIA HR 4040 Compliant Linear trimellitate esterContains 0.10-0.15 wt% 1,1,3-Tris (2-methyl-4hydroxy-5-t-butyl phenyl) butane antioxidantInformation provided by PolyOne |
|||
Kinematic Viscosity at 40°C (104°F) | 45 cSt | 45 cSt | |
ConocoPhillips Hydroclear® 1 Ultra-clean multi-purpose R&O Oil, AGMA Lubricant No. 1 Description: Conoco Hydroclear Ultra-Clean Multipurpose R&O Oil is a rust- and oxidation-inhibited industrial oil with ashless wear protection formulated from premium Conoco hydrocracked base stocks.. |
|||
Kinematic Viscosity at 40°C (104°F) | 45 cSt | 45 cSt | |
ConocoPhillips Hydroclear® 46 Multipurpose R&O Oil, AGMA Lubricant No. 1 Description: Conoco Hydroclear Multipurpose R&O Oil is a rust- and oxidation inhibited industrial oil with ashless wear protection formulated from premium Conoco hydrocracked base stocks. Hydroclear.. |
|||
Kinematic Viscosity at 40°C (104°F) | 45 cSt | 45 cSt | |
ConocoPhillips Hydroclear® 46 Turbine Oil Description: Conoco Hydroclear Turbine Oil is a premium rust- and oxidationinhibited turbine oil formulated from exclusive Conoco hydrocracked base stock. Hydroclear Turbine Oil is specially formula.. |