Physical Properties | Metric | English | Comments |
---|---|---|---|
Kinematic Viscosity at 40°C (104°F) | 43 cSt | 43 cSt | Base Oil; ASTM D445 |
Nye Lubricants 802-1 (FG) Synthetic Oil Information provided by Nye Lubricants. |
|||
Kinematic Viscosity at 40°C (104°F) | 43 cSt | 43 cSt | ASTM D445 |
ExxonMobil Mobil 1 0W-20 Mobil 1 W-20, Power and Performance Formula, is the most advanced performance synthetic engine oil designed to provide the ultimate level of power, and protection to keep engines running smoothly an.. |
|||
Kinematic Viscosity at 40°C (104°F) | 43 cSt | 43 cSt | ASTM D445 |
ChevronTexaco 220R Neutral Oil FeaturesChevron Neutral Oils are all-hydroprocessed, highly refined API Group II paraffinic base stocks. Their extremely low sulfur, nitrogen, and aromatic content give them excellent thermal and o.. |
|||
Kinematic Viscosity at 40°C (104°F) | 43 cSt | 43 cSt | |
ConocoPhillips Hydroclear® ATF Type F Automatic Transmission Fluid Description: Conoco Hydroclear ATF Type F Automatic Transmission Fluid is a high-static-friction fluid developed for Ford automatic transmissions manufactured during the 1960s and 1970s. (Newer Ford.. |
|||
Kinematic Viscosity at 40°C (104°F) | 43 cSt | 43 cSt | ASTM D445 |
ExxonMobil Mobil 1 0W-20 Mobil 1 W-20, Power and Performance Formula, is the most advanced performance synthetic engine oil designed to provide the ultimate level of power, and protection to keep engines running smoothly an.. |